| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Particle Size | <= 30 µm | <= 30 µm | 90% smaller than |
|
Nyco M400 WOLLASTOCOAT® Wollastonite
Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per..
|
|||
| Particle Size | 30 - 50 µm | 30 - 50 µm | Mean |
|
Potters Industries Spheriglass® 3000 Solid Glass Spheres
Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage..
|
|||
| Particle Size | 30 - 70 µm | 30 - 70 µm | d50 |
|
Magyar Aluminum ALO-P54 Alumina
Alumina for Polishing
|
|||
| Particle Size | <= 30 µm | <= 30 µm | 99% finer |
|
Malvern Minerals Novacite® 1250 Untreated Lamellar Quartz Filler/Extender
Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo..
|
|||
| Particle Size | <= 30 µm | <= 30 µm | 99% finer |
|
Malvern Minerals Novakup® 1250 Surface-Treated Lamellar Quartz Filler/Extender
Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen..
|
|||
| Particle Size | 30 µm | 30 µm | 75% finer than |
|
Imerys Minsilsparâ„¢ Feldspar
Minsilspar is a 170 mesh feldspathic sand (sandspar) used primarily in the Sanitaryware industry.Information provided by Imerys
|
|||
| Particle Size | 30 - 38 µm | 30 - 38 µm | 50% |
|
H.C. Starck Amperit® 519.074 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO) |
|||
| Particle Size | 30 - 40 µm | 30 - 40 µm | 90% |
|
H.C. Starck Amperit® 588.059 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) |
|||
| Particle Size | 30 - 40 µm | 30 - 40 µm | 50% |
|
H.C. Starck Amperit® 832.054 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
| Particle Size | 30 - 37 µm | 30 - 37 µm | |
|
H.C. Starck Amperit® 146.3 Chromium (Cr)
HS Number: 81122031
|
|||
| Particle Size | 30 µm | 30 µm | 95%, Laser diffraction; QSOP-5&75 |
|
Shamrock Technologies Fluoro T® 607 Thermoplastic Grade PTFE Additive
The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction ..
|
|||
| Particle Size | 30 µm | 30 µm | 95%, Laser diffraction; QSOP-5&75 |
|
Shamrock Technologies Fluoro T® 807 Thermoplastic Grade PTFE Additive
The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction ..
|
|||
| Particle Size | 30 µm | 30 µm | |
|
Silberline Extra Sparkle Silvex® 400-10-C
Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited ..
|
|||
| Particle Size | 30 µm | 30 µm | |
|
Silberline Sparkle Silver® 3166-AR
Sparkle Silver® 3166-AR is a coarse high sparkle, non-leafing aluminum pigment popular for Automotive Applications. This pigment can be used with tints to produce a wide range of polychromatic ef..
|
|||
| Particle Size | 30 µm | 30 µm | |
|
Silberline Sparkle Silver® 3666
Sparkle Silver® 3666 is a coarse, bright, regular purity, non-leafing aluminum pigment popular for solvent-based general industrial coatings. This pigment can be used with tints to produce a wide..
|
|||
| Particle Size | 30 µm | 30 µm | 99.5% less than value (Size D) |
|
Vesta Ceramics SicoMill® Grade 2 Silicon Powder
General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu..
|
|||
| Particle Size | 30 µm | 30 µm | 98% less than value (Size C) |
|
Vesta Ceramics SicoMill® Grade 4 Silicon Powder
General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu..
|
|||
| Particle Size | 30 µm | 30 µm | 99.5% less than value (Size D) |
|
Vesta Ceramics SicoMill® Grade 4 Silicon Powder
General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu..
|
|||
| Particle Size | 30 µm | 30 µm | @ 98% |
|
CIMBAR Body Filler Talc for Polyester Filler
Gel Talc and Body Filler talc products are produced from high purity ore. Gel Talc and Body Filler products provide an excellent balance of color and mechanical properties for primary use in polyes..
|
|||
| Particle Size | 30 µm | 30 µm | @ 98%; Micrometrics Sedigraph 5100 |
|
CIMBAR RP 9310 Talc
RP 9300 Series talcs are produced from high purity ores, which provide an excellent balance of color and mechanical properties, for primary use in commodity polypropylene and polyester compounds. R..
|
|||
| Particle Size | 30 - 50 µm | 30 - 50 µm | D(0.5) |
|
Akzo Nobel Expancel® 551 DE 40 d42 Dry expanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Particle Size | 30 - 50 µm | 30 - 50 µm | D(0.5) |
|
Akzo Nobel Expancel® 551 WE 40 d36 Wet expanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Particle Size | 30 µm | 30 µm | 90th% |
|
3M iM16K Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
|
|||
| Particle Size | 30 µm | 30 µm | 10th% |
|
3M K20 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
|
|||
| Particle Size | 30 µm | 30 µm | Average diameter |
|
3M Scotchlite™ S60/10000 Glass Bubbles
High-strength polymer additives made from a water-resistant and chemically-stable soda-lime-borosilicate glass. These hollow glass microspheres can be used as a low density filler material ideal for..
|
|||
| Particle Size | 30 µm | 30 µm | |
|
3M Dyneon™ PFA 6503PBZ Fluoroplastic Powder
3M™ Dyneon™ Fluoroplastic Powder PFA 6503PBZ is a fluorothermoplastic powder with excellent thermal stability characteristics, designed for use in thin film powder coatings. Typical applications i..
|
|||
| Particle Size | 30 µm | 30 µm | 50th% |
|
3M S60 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
|
|||
| Particle Size | 30 - 100 µm | 30 - 100 µm | D10-D90 |
|
ALM PA 606-FR Filled Nylon 12 Prototyping Polymer
Only commercially available fire retardant nylon 12 material, which meets FAR 25.853 60 second burn specification.The parts produced from PA 606-FR have a much smoother surface finish and sharper fe..
|
|||
| Particle Size | 30 µm | 30 µm | median |
|
3M Dyneon™ PFA 6503 B EPC Perfluoroalkoxy Fluorothermoplastic
(discontinued **)
Dyneon PFA 6503 B EPC is a fluorothermoplastic powder for powder coating applications, and is designed for thin film applications where target film thickness is 25-40 micrometers per pass.non-stick ..
|
|||
| Particle Size | 30 - 50 µm | 30 - 50 µm | mean value |
|
Potters Industries Spheriglass® 3000E Solid Glass Spheres
Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage..
|
|||