Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage = 0.012 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Multibase Nylex™ 2185 HFX Natural Polyamide + PP
Forms: PelletsProcessing Methods:Injection moldingFeatures:Tensile Strength, HighInformation provided by Multibase
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Multibase Nylex™ 2185 R15 Polyamide + PP
Glass fiber reinforcement, 15% Filler by Weight. Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Metho..
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
RheTech Products M12P100-01 12% Mica Reinforced Polypropylene, Black
Applications: Fan shroudsAir ductsFiller panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
Nylene® 321 (HS) Impact Modified Nylon 6
Description: Nylene® 321 (HS) is an impact modified nylon 6. Information provided by Custom Resins.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporatio..
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
RheTech Products T20P100-00 20% Talc Reinforced Polypropylene, Natural
Applications: Electronic housingsConsolesIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products..
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
RheTech Products T20P100-01UV 20% Talc Reinforced Polypropylene, UV Stabilized, General Purpose Black
Applications: Durable goodsElectronics housingsIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
RheTech Products T20P104-01 20% Talc Reinforced Polypropylene, Black
Applications: Electronic housingsIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
Across Flow; ISO 2577
Polykemi AB SCANAMID 66 A33^E F15 Nylon 66, Glass Fiber Reinforced, Modified
Information provided by Polykemi AB
Linear Mold Shrinkage 0.012 - 0.014 cm/cm
0.012 - 0.014 in/in
With Flow; ISO 2577
Polykemi AB POLYfill PPC BGK601213 CR Polypropylene Copolymer, Multifiller
Information provided by Polykemi AB
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
0.125 in; ASTM D955
Ravago Manufacturing Americas Hylon® N1000NL Nylon 6/6 (DAM)  (discontinued **)
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
MD; ASTM Test
BASF Capron® 8200 NL Nylon 6 (Conditioned)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Linear Mold Shrinkage 0.012 - 0.018 cm/cm

@Thickness 1.60 mm
0.012 - 0.018 in/in

@Thickness 0.0630 in
ASTM D955
Gromax PBT 1100-211H
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Multibase Multi-Flex® D 4400 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good F..
Linear Mold Shrinkage 0.012 - 0.014 cm/cm

@Temperature 23.0 °C
0.012 - 0.014 in/in

@Temperature 73.4 °F
ASTM D955
Kingfa PBT-R0N Flame Retardant PBT
Features:Flame retardantGood chemical resistanceOutstanding surfaceEasy processingHigh impactApplications:Injection moldingConnectors, terminal blocksRelay, switchBobbinsPlugsE & E partsInformation ..
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
LG Chemical LUPOL HM-5204B High Modulus Polypropylene, 20% Polymer Alloy, High Strength, High Flow, High Modulus
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
Linear Mold Shrinkage 0.012 cm/cm

@Thickness 3.17 mm
0.012 in/in

@Thickness 0.125 in
Shakespeare Isocorâ„¢ HG26SI medium viscosity PA-612
Isocorâ„¢ HG26SI is a medium viscosity PA-612 based nylon. This resin is specifically suited for applications requiring low moisture regain and greater dimensional stability. Isocorâ„¢ HG2..
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
0.125inch wall
Spartech PP5230 Calcium Carbonate Filled Homopolymer
Offers improved stiffness versus unfilled materials. They offer substantial improvements in drop weight (Gardner) impact over both unfilled polypropylene and other types of filled polypropylene. Cal..
Linear Mold Shrinkage 0.012 - 0.014 cm/cm
0.012 - 0.014 in/in
ASTM D955
Samyang Tribit® 1500A15 PBT, Inorganic Reinforced
Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500A15 contains inorganic filler.Applicati..
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Teknor Apex Monprene® MP-2132 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Linear Mold Shrinkage <= 0.012 cm/cm
<= 0.012 in/in
Voloknohim Filament Nylon Linear Density 117 tex
Application: for production of goods for fishery and for other technical purposes. The produced yarn is bright, UV-stabilized, thermostabilized, UV-thermostabilized, not dyed, dyedInformation provi..
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
± 0.1 after 30 min. at 120°C
A. Schulman POLYTROPE™ TPP 518 Injection Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 518 is an injection grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal expansion i..
Linear Mold Shrinkage 0.012 - 0.016 cm/cm
0.012 - 0.016 in/in
Polyram PlusTek PB300G3 Nylon 6, 15% Glass Fiber
15% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.012 - 0.014 cm/cm
0.012 - 0.014 in/in
ASTM D 955
Cossa Polimeri ESTAPROP 1040 V2 H Flame Retardant Polypropylene
PP homopolymerFlame retardant class V2, halogen free, good mechanical characteristicsInformation provided by Cossa Polimeri S.r.l.
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
Eurotec® Tecomid® NA40 NL XA 20 PA 6.6 unreinforced, UL94 V0
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM Data; MD
BASF Ultramid® 8202 HS BK-102 PA6 (Conditioned)
Ultramid 8202 HS BK-102 is an unfilled, heat stabilized, pigmented black, low viscosity, general purpose injection molding PA6 exhibiting excellent fluidity for filling thin sections. It possesses ..
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
MD; ASTM D955
Aclo Accucomp Polypropylene HPO309L Homopolymer
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
STN EN ISO 294-4
Plastcom SLOVALEN PH 69 GF 30/1M Polypropylene reinforced with glass fiber
Modified homopolymer PP for injection molding, reinforced with 30% glass fiber. Applied in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Pl..
Linear Mold Shrinkage 0.012 cm/cm

@Thickness 1.59 mm
0.012 in/in

@Thickness 0.0625 in
ASTM D955
Plastics Group Polifil® RMT-20V 20% Talc-Reinforced Polypropylene, High Impact, UV Stabilized
Polifil® RMT-V series compounds are high impact, UV stabilized polypropylenes reinforced with asbestos-free talc. In addition to high impact strength, they possess a high flex modulus and the abili..
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Buckeye Polymers BP RPP 1010 TR Blk Reprocessed Polypropylene, 10% Mineral Filled
Talc Filled BlackThis reprocessed product is successful in applications where cost is a major specification, yet physical characteristics require product performance. Industrial recycled resin comp..