| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | ASTM D955 |
|
Multibase Multi-Pro® 1008 T Polypropylene
Talc Filler, 10% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
|
|||
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | ASTM D955 |
|
Multibase Nylex™ 2185 R15 Polyamide + PP
Glass fiber reinforcement, 15% Filler by Weight. Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Metho..
|
|||
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | |
|
Plastcom SLOVALEN PH 49 GF 10 GB 20 PP, 20% glass beads, 10% glass fibre, coupling agent
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10 % glass fiber and 20% glass beads, contains themodifier of mechanical properties. Increased strength in comparis..
|
|||
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | ASTM D955 |
|
RheTech Products FT4900-772UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black
Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | ASTM D955 |
|
RheTech Products T20P100-517UV 20% Talc Reinforced Polypropylene, UV Stabilized, Interior DX9 Black
Applications: Center consolesIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | Across Flow; ISO 2577 |
|
Polykemi AB POLYshine PBT D231 GF30 PBT, Glass-Fiber Reinforced
Information provided by Polykemi AB
|
|||
| Linear Mold Shrinkage | 0.012 - 0.020 cm/cm | 0.012 - 0.020 in/in | FRISETTA Test Method |
|
Nilit FRIANYL B63 SI20 Nylon 6 for injection molding
Nylon 6 for injection molding, ionomer impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | ASTM D955 |
|
Global TPP-120 20% Talc Filled Polypropylene
Information provided by Global Polymers Corporation.
|
|||
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | ASTM D955 |
|
Multibase Multi-Flex® D 5308 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, GoodScratch Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automot..
|
|||
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | ASTM D955 |
|
Multibase Multi-Flex® A 7727 TLC Black TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
|
|||
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | ASTM D955 |
|
Teknor Apex Monprene® MP 1023 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Linear Mold Shrinkage | 0.012 - 0.014 cm/cm | 0.012 - 0.014 in/in | ASTM D955 |
|
PlastxWorld CEVIAN® B1700 PBT/ABS Alloy
Unfilled, High Heat ResistantThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
|
|||
| Linear Mold Shrinkage | <= 0.012 cm/cm | <= 0.012 in/in | |
|
Voloknohim Filament Nylon Linear Density 140 tex
Application: for production of goods for fishery and for other technical purposes. The produced yarn is bright, UV-stabilized, thermostabilized, UV-thermostabilized, not dyed, dyedInformation provi..
|
|||
| Linear Mold Shrinkage | <= 0.012 cm/cm | <= 0.012 in/in | |
|
Voloknohim Filament Nylon Linear Density 70 tex
Application: for production of goods for fishery and for other technical purposes. The produced yarn is bright, UV-stabilized, thermostabilized, UV-thermostabilized, not dyed, dyedInformation provi..
|
|||
| Linear Mold Shrinkage | 0.012 - 0.025 cm/cm | 0.012 - 0.025 in/in | |
|
Polyram RamOfin RPPC711 Polypropylene, UV Stabilized
UV stabilized polypropylene copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | MD; ASTM D955 |
|
Aclo Accutech Polypropylene Copolymer CP0436C10L Calcium Reinforced |
|||
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | MD; ASTM D955 |
|
Aclo Accutech Polypropylene Copolymer CP0437T10L Talc Reinforced |
|||
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | MD; ASTM D955 |
|
Aclo Accutech Polypropylene Homopolymer HP0334T10L Talc Reinforced |
|||
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | ASTM D955 |
|
Buckeye Polymers BP Flex A9505 TPO
TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a..
|
|||
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | ASTM Data; MD |
|
BASF Ultramid® 8202 PA6 (Conditioned)
Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult..
|
|||
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | Injection; ASTM D955 |
|
Chang Chun Plastic Longlite PM T373J Electrical Phenolic Molding Compound
ASTM Grades per ASTM D700 are 2, 3.Information provided by Dowell Trading Company Ltd.
|
|||
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | ASTM D955 |
|
A. Schulman ComAlloy Comtuf® 652 Nylon 6/6, Mineral Reinforced, Impact Modified
Data provided by the manufacturer, ComAlloy International Company.30% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i..
|
|||
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | ASTM D955 |
|
Aaron Industries AAROPRENE® CFIPP 2010 High Impact Calcium Carbonate Filled Polypropylene
AAROPRENE® CFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified.
|
|||
| Linear Mold Shrinkage |
0.012
-
0.018
cm/cm @Thickness 1.60 mm |
0.012
-
0.018
in/in @Thickness 0.0630 in |
ASTM D955 |
|
Gromax PBT 1200-211D
Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle..
|
|||
| Linear Mold Shrinkage | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | after bake; ISO 294 |
|
Solvay Engineered Polymers DEXFLEX® 880 TPO
(discontinued **)
Description: DEXFLEX® 880 is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, low-temperature impact, good processabil..
|
|||
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | ASTM D955 |
|
PolyOne Synprene® IT 584 Thermoplastic Elastomer - SBC
(discontinued **)
Description/Features:High Performance Thermoplastic ElastomerOpaqueApplications:Multi-PurposeFDA (Food Contact)Processing Method:Injection MoldingPolyOne First ChoiceDisclaimer: A thermoplastic elas..
|
|||