| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.40 g/cc | 0.0506 lb/in³ | DAM; ISO 1183 |
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm @Thickness 2.00 mm |
0.0030 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.0070 cm/cm @Thickness 2.00 mm |
0.0070 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 200 MPa @Temperature 23.0 °C |
29000 psi @Temperature 73.4 °F |
DAM; ISO 527 |
| Elongation at Break | 3.5 % @Temperature 23.0 °C |
3.5 % @Temperature 73.4 °F |
DAM; ISO 527 |
| Tensile Modulus | 11.0 GPa @Temperature 23.0 °C |
1600 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
| Flexural Modulus | 10.0 GPa @Temperature 23.0 °C |
1450 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
| Izod Impact, Notched (ISO) | 13.0 kJ/m² @Temperature -40.0 °C |
6.19 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A |
| 15.0 kJ/m² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A | |
| Charpy Impact, Notched | 1.20 J/cm² @Temperature -40.0 °C |
5.71 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 179/1eA |
| 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 260 °C | 500 °F | 10°C/min; DAM; ISO 11357-1/-3 |
| Deflection Temperature at 1.8 MPa (264 psi) | 250 °C | 482 °F | DAM; ISO 75-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 2.00e+18 ohm-cm @Temperature 23.0 °C |
2.00e+18 ohm-cm @Temperature 73.4 °F |
DAM; IEC 60093 |
| Surface Resistance | 4.00e+15 ohm @Temperature 23.0 °C |
4.00e+15 ohm @Temperature 73.4 °F |
DAM; IEC 60093 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 295 °C | 563 °F | DAM; Optimum |
| 285 - 305 °C | 545 - 581 °F | DAM | |
| Mold Temperature | 70.0 - 120 °C | 158 - 248 °F | DAM |
| 100 °C | 212 °F | DAM; optimum | |
| Drying Temperature | 80.0 °C | 176 °F | DAM |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM |
| Moisture Content | <= 0.20 % | <= 0.20 % | DAM |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Natural Color | DAM |
| Forms | Pellets | DAM |
| Generic | Nylon 66 | DAM |
| Material Status | Preliminary Data | DAM |
| Part Marking Code | >PA66-GF35< | ISO 11469; DAM |
| Processing Method | Injection Molding | DAM |
| Product Category | Electrical Resins | DAM |
| Encapsulation Resins | DAM | |
| Glass Reinforced Resins | DAM | |
| Region Available - Global | Yes | DAM |
| Resin Identification | PA66-GF35 | ISO 1043; DAM |
| RoHS Compliance | Contact Manufacturer | DAM |