| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Flow | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | ASTM D955 |
|
PolyOne LubriOne™ AT-000/18T 2S Acetal (POM) Copolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
|
|||
| Linear Mold Shrinkage, Flow | 0.020 - 0.023 cm/cm | 0.020 - 0.023 in/in | ASTM D955 |
|
PolyOne LubriOne™ ATH-000/18T 2S Acetal (POM) Homopolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
|
|||
| Linear Mold Shrinkage, Flow |
0.020
-
0.040
cm/cm @Thickness 3.18 mm |
0.020
-
0.040
in/in @Thickness 0.125 in |
ASTM D955 |
|
PolyOne Stat-Tech™ NN-40CF/000 FRV0 Natural Polyamide 66 (Nylon 66)
Information provided by PolyOne
|
|||
| Linear Mold Shrinkage, Flow | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | |
|
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF)
(Unverified Data**)
Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers.
|
|||
| Linear Mold Shrinkage, Flow |
0.020
cm/cm @Time 86400 sec |
0.020
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP KAL22XXC Acetal Copolymer
LNP* LUBRICOMP* KAL22XXC is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid. Added feature of this material is: Wear Resistant.
|
|||
| Linear Mold Shrinkage, Flow |
>=
0.020
cm/cm @Time 86400 sec |
>=
0.020
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP RAP22 PA 66
LNP* LUBRICOMP* RAP22 is a compound based on Nylon 66 resin containing 10% Aramid, 10% PTFE/Silicone. Added feature of this grade includes: Wear Resistant.
|
|||
| Linear Mold Shrinkage, Flow |
>=
0.020
cm/cm @Time 86400 sec |
>=
0.020
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP WI001 PBT
LNP* LUBRICOMP* WI001 is a compound based on PBT containing 2% Silicone. Added feature of this grade is: Wear Resistant.
|
|||
| Linear Mold Shrinkage, Flow |
>=
0.020
cm/cm @Time 86400 sec |
>=
0.020
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRILOY RA2 PA 66
LNP* LUBRILOY* RA2 is a compound based on Nylon 66 resin containing Aramid Fiber. Added feature of this material is: Wear Resistant.
|
|||
| Linear Mold Shrinkage, Flow | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | |
|
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF)
Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Features: Homopolymer; Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3417 54.0 to 6..
|
|||
| Linear Mold Shrinkage, Flow |
>=
0.020
cm/cm @Time 86400 sec |
>=
0.020
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP STAT-KON IS000XXL PA6.12
LNP* STAT-KON* IS000XXL is a compound based on Nylon 6/12 containing Stainless Steel Fibers. Added features of this material include: Food Contact Compliant Raw Materials, Metal Detectable, Electr..
|
|||
| Linear Mold Shrinkage, Flow |
0.020
cm/cm @Thickness 3.17 mm |
0.020
in/in @Thickness 0.125 in |
ASTM D955 |
|
Techmer ES HiFill® PBT 620
Availability: North AmericaForms: PelletsFeatures: Medium FlowAppearance: Natural ColorInformation provided by TP Composites, Inc.
|
|||
| Linear Mold Shrinkage, Flow |
>=
0.020
cm/cm @Time 86400 sec |
>=
0.020
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP THERMOCOMP WH0200B PBT
LNP* Thermocomp* WH0200B is a compound based on PBT resin containing proprietary fillers. Added features include: High Specific Gravity.
|
|||
| Linear Mold Shrinkage, Flow |
>=
0.020
cm/cm @Time 86400 sec |
>=
0.020
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP STAT-KON RD000I PA 66
LNP* STAT-KON* RD000I is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
|
|||
| Linear Mold Shrinkage, Flow |
>=
0.020
cm/cm @Time 86400 sec |
>=
0.020
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP STAT-LOY W3000XXJ PBT
LNP* STAT-LOY* W3000XXJ is a compound based on PBT. Added features of this grade include: Anti-Stat, Colorable, Healthcare
|
|||
| Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | SABIC Method |
|
SABIC Innovative Plastics LNP Thermocomp WB006 PBT (Europe-Africa-Middle East)
LNP* THERMOCOMP* WB006 is a compound based on Polybutylene Terephalate resin containing Glass Bead.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | DAM; ISO 294-4 |
|
DSM Stanyl® TE341 Nylon 46 (European Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | ISO 294-4 2577 |
|
DuPont Performance Polymers Delrin® 527UVE RD402 Acetal (POM)
(Unverified Data**)
UV Stabilized Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 527UVE RD402 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers pigmented red with very ..
|
|||
| Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | ISO 294-4 2577 |
|
DuPont Performance Polymers Delrin® 500PE BK602 Acetal (POM)
(Unverified Data**)
Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE BK602 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi..
|
|||
| Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | ISO 294-4 |
|
Barlog Plastics KEBAFORM C 270 LS black POM Copolymer unreinforced, laser markable
POMInformation provided by BARLOG plastics GmbH.
|
|||
| Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | ISO 294-4 |
|
Barlog Plastics KEBAFORM C 270.0 POM Copolymer unreinforced
POMInformation provided by BARLOG plastics GmbH.
|
|||
| Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | ISO 294-4 |
|
Barlog Plastics KEBAFORM C 901 MS POM Copolymer unreinforced, improved wear and friction
POMInformation provided by BARLOG plastics GmbH.
|
|||
| Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | ISO 294-4 |
|
Barlog Plastics KEBAFORM C 909 WR POM Copolymer unreinforced, UV-stabilized
POMInformation provided by BARLOG plastics GmbH.
|
|||
| Linear Mold Shrinkage, Flow |
0.020
cm/cm @Diameter 2.00 mm |
0.020
in/in @Diameter 0.0787 in |
ISO 294-4 |
|
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, Conditioned
Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit..
|
|||
| Linear Mold Shrinkage, Flow |
0.020
cm/cm @Diameter 2.00 mm |
0.020
in/in @Diameter 0.0787 in |
ISO 294-4 |
|
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM
Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit..
|
|||
| Linear Mold Shrinkage, Flow | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | |
|
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF)
(Unverified Data**)
Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Information provided by Solvay Specialty Polymers.
|
|||
| Linear Mold Shrinkage, Flow |
0.020
cm/cm @Thickness 3.17 mm |
0.020
in/in @Thickness 0.125 in |
ASTM D955 |
|
Techmer ES HiFill® TPX-HTN-01043 A
Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: High Temperature Strength, Impact Modified and LubricatedUL File Number: E157318Information provided by TP C..
|
|||
| Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | Sim. To ISO 294-4 |
|
DSM Arnite® T06 204 XL PBT
Low Viscosity, Injection Molding, Low outgassing
|
|||
| Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | Sim. To ISO 294-4 |
|
DSM Stanyl® TE300 PA46
Heat Stabilized
|
|||