| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Flow | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | ASTM D955 |
|
PolyOne LubriOne™ AT-000/20T Black Acetal (POM) Copolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
|
|||
| Linear Mold Shrinkage, Flow | 0.020 - 0.023 cm/cm | 0.020 - 0.023 in/in | ASTM D955 |
|
PolyOne LubriOne™ ATH-XC-361E Acetal (POM) Homopolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
|
|||
| Linear Mold Shrinkage, Flow |
0.020
-
0.040
cm/cm @Thickness 3.18 mm |
0.020
-
0.040
in/in @Thickness 0.125 in |
ASTM D955 |
|
PolyOne Edgetek® NN-40CF/000 FRV0 NATURAL Polyamide 66 (Nylon 66)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
|
|||
| Linear Mold Shrinkage, Flow | 0.020 - 0.023 cm/cm | 0.020 - 0.023 in/in | |
|
LATI Latilub 73/13-01M POM, Molybdenum disulphide Filled
Self-lubricating product based on Polyoxymethylene (POM). Molybdenum disulphide. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati In..
|
|||
| Linear Mold Shrinkage, Flow |
0.020
cm/cm @Time 86400 sec |
0.020
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE (Asia Pacific)
LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Flow |
0.020
cm/cm @Time 86400 sec |
0.020
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP KAL22XXC Acetal Copolymer
LNP* LUBRICOMP* KAL22XXC is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid. Added feature of this material is: Wear Resistant.
|
|||
| Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | SABIC Method |
|
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer (Europe-Africa-Middle East)
LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer containing Graphite. Added features include : Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Flow |
>=
0.020
cm/cm @Time 86400 sec |
>=
0.020
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP KL003LH Acetal
LNP* LUBRICOMP* KL003LH is an Acetal based compound containing 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant.
|
|||
| Linear Mold Shrinkage, Flow |
>=
0.020
cm/cm @Time 86400 sec |
>=
0.020
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP KX06415 Acetal Copolymer
LNP LUBRICOMP* KX06415 is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid Powder. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant.
|
|||
| Linear Mold Shrinkage, Flow |
>=
0.020
cm/cm @Time 86400 sec |
>=
0.020
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP ML004S PP
LNP* LUBRICOMP* ML004S is a compound based on Polypropylene resin containing 20% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized.
|
|||
| Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | SABIC Method |
|
SABIC Innovative Plastics LNP LUBRICOMP ML008 PP (Europe-Africa-Middle East)
LNP* LUBRICOMP* ML008 is a compound based on Polypropylene resin containing PTFE. Added Features include: Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Flow |
0.020
-
0.040
cm/cm @Time 86400 sec |
0.020
-
0.040
in/in @Time 24.0 hour |
ASTM D 955 |
|
SABIC Innovative Plastics LNP Lubricomp RL001 PA 66
LNP Lubricomp* RL001 is a Nylon 6/6 base resin containing PTFE lubricant. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Linear Mold Shrinkage, Flow |
>=
0.020
cm/cm @Time 86400 sec |
>=
0.020
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP RX88514 PA 66
LNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). AddedLNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). A..
|
|||
| Linear Mold Shrinkage, Flow | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | |
|
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)
Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D..
|
|||
| Linear Mold Shrinkage, Flow | 0.020 - 0.030 cm/cm | 0.020 - 0.030 in/in | |
|
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF)
Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Features: Homopolymer; Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3417 54.0 to 6..
|
|||
| Linear Mold Shrinkage, Flow |
0.020
cm/cm @Thickness 3.17 mm |
0.020
in/in @Thickness 0.125 in |
ASTM D955 |
|
Techmer ES Luriblend® POM HO TL2 Acetal
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(2%)Features: Lubricated, Good Wear Resistance and HomopolymerInformation provided by TP Composites, Inc.
|
|||
| Linear Mold Shrinkage, Flow |
>=
0.020
cm/cm @Time 86400 sec |
>=
0.020
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP STAT-LOY M3000C PP
LNP* STAT-LOY* M3000C is a compound based on unfilled Polypropylene resin. Added features of this grade include: Clean Compound System, Antistat.
|
|||
| Linear Mold Shrinkage, Flow |
>=
0.020
cm/cm @Time 86400 sec |
>=
0.020
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP THERMOTUF VF1001S Super Tough Nylon
LNP* Thermotuf* VF1001S is a Super Tough Nylon containing glass fiber. Characteristics of this grade is Heat Stabilized.
|
|||
| Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | DAM; ISO 294-4 |
|
DSM Stanyl® TW300 Nylon 46 (European and Asian Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | ISO 294-4 2577 |
|
DuPont Performance Polymers Delrin® 300PE BK602 Acetal (POM)
(Unverified Data**)
Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE BK602 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low..
|
|||
| Linear Mold Shrinkage, Flow |
0.020
cm/cm @Thickness 2.00 mm |
0.020
in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
|
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66
(Unverified Data**)
Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf..
|
|||
| Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | ASTM D955 |
|
Clariant Renol PA133 Nylon 66, Highly Impact Modified, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | DAM; ISO 294-4 |
|
DSM Stanyl® TW363 Nylon 46 (European Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | ISO 294-4 2577 |
|
DuPont Performance Polymers Delrin® 500PE BK602 Acetal (POM)
(Unverified Data**)
Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE BK602 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi..
|
|||
| Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | ISO 294-4 |
|
Barlog Plastics KEBAFORM C 270 LS black POM Copolymer unreinforced, laser markable
POMInformation provided by BARLOG plastics GmbH.
|
|||
| Linear Mold Shrinkage, Flow | 0.020 cm/cm | 0.020 in/in | ISO 294-4 |
|
Barlog Plastics KEBAFORM C 906 LF POM Copolymer unreinforced, improved wear and friction
POMInformation provided by BARLOG plastics GmbH.
|
|||
| Linear Mold Shrinkage, Flow |
0.020
cm/cm @Diameter 2.00 mm |
0.020
in/in @Diameter 0.0787 in |
ISO 294-4 |
|
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned
Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance..
|
|||
| Linear Mold Shrinkage, Flow |
>=
0.020
cm/cm @Time 86400 sec |
>=
0.020
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP THERMOCOMP WF002I PBT
LNP* THERMOTUF* WF006I is a compound based on PBT resin containing 10% Glass Fiber. Added feature of this grade is: High Impact.
|
|||