Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Transverse = 0.013 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
Euronil
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer
Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr..
Linear Mold Shrinkage, Transverse 0.013 cm/cm

@Time 86400 sec
0.013 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP FARADEX MS003 PP (Asia Pacific)
LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Linear Mold Shrinkage, Transverse 0.013 cm/cm

@Time 86400 sec
0.013 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP FARADEX MS003 PP (Europe-Africa-Middle East)
LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Linear Mold Shrinkage, Transverse 0.013 - 0.015 cm/cm

@Thickness 3.18 mm
0.013 - 0.015 in/in

@Thickness 0.125 in
5" x 0.5" x 0.125" bars; ASTM D955
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 resin. ..
Linear Mold Shrinkage, Transverse 0.013 - 0.015 cm/cm

@Thickness 3.18 mm
0.013 - 0.015 in/in

@Thickness 0.125 in
5" x 0.5" x 0.125"; ASTM D955
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire..
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
Euronil
Nilit Nilamid A3 H ZC High Impact PA66
Description: Nilamid A3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, ..
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
Euronil
Nilit Nilamid A3 H ZE High Impact PA66
Description: Nilamid A3 H ZE was developed for applications which are subjected to very high shock loads, also at minus temperatures. It has good impact performance, whilst maintaining good strength..
Linear Mold Shrinkage, Transverse 0.013 cm/cm

@Thickness 2.00 mm
0.013 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66  (Unverified Data**)
Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Transverse 0.013 - 0.015 cm/cm
0.013 - 0.015 in/in
ASTM D955
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and..
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
ASTM D955
Teknor Apex Monprene® MP 1187 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
ISO 294-4
DSM EcoPaXX® Q-PG6 PA410-I-GF30
% Glass Reinforced, Impact Modified
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
ISO 294-4, 2577
EMS-Grivory Grivory® BS PA6
Product description: Grilon BS is an unreinforced, heat stabilized standard PA6 injection molding grade with normal melt viscosity. Grilon BS has the following important properties: Good flow behavi..
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
ISO 294-4
DSM Stanyl® TW200F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
Eurotec
Eurotec® Tecomid® NA40 GR14 NL MC PA6.6, 14% glass fiber reinforced, impact modified, heat stabilized, natural
Information provided by Eurotec®
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
ISO 294-4
DSM EcoPaXX® Q150-D PA410
Low/Medium Viscosity
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
ISO 294-4, 2577
EMS-Grivory Grivory® L 25 Z PA12-I
Product Description: Grilamid L 25 Z is a UV- and heat stabilized high viscosity polyamide 12 grade with improved toughness. A special feature of Grilamid L25 Z is its high energy absorption capacit..
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
DAM; ISO 294-4 2577
DuPont Performance Polymers Zytel® 103FHS BKB038 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS BKB038 is a heat stabilized lubricated PA 66 resin for fast cycling.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
DAM; ISO 294-4 2577
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66  (Unverified Data**)
Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe..
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
Eurotec® Tecomid® NB40 NL IL PA 6 impact modified
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
E-Polymers TEKAMID® JN2 PPE+PA66 Un-reinforced Chemical resistance PA/PPE Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P..
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
ISO 294-4
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Dry, 30% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
ISO 294-4
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Conditioned, 35% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
Advanced Polymer Alloys DuraGrip™ DGR 6050 NC/BK Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6050 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6050 NC/BK have an excellent soft t..
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
ISO 294-4
Barlog Plastics KEBAFLEX S 25 A.01 TPE-S, Shore A25, translucent
TPE-SInformation provided by BARLOG plastics GmbH.
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
DAM; ISO 294-4 2577
DuPont Performance Polymers Zytel® 103FHS BKB009 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS BKB009 is a heat stabilized internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productiv..
Linear Mold Shrinkage, Transverse 0.013 - 0.0165 cm/cm
0.013 - 0.0165 in/in
LATI Latiohm 66-10 H2 CNT CE/10 PA66, 10% Mineral Fiber Reinforced, Heat Stabilized
Semiconductive/dissipative product based on Polyamide 66 (PA66). Heat stabilized. Carbon nanotubes. Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame..
Linear Mold Shrinkage, Transverse 0.013 - 0.017 cm/cm
0.013 - 0.017 in/in
ISO DIS 294-4
Wellman Wellamid® 42LH-NBK1 General Purpose Nylon 6
Description: General Purpose Nylon 6Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
E-Polymers TEKAMID® JN1 PPE+PA66 Un-reinforced High flow Heat resistance PA/PPE Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P..
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
ISO 2577
BASF Ultradur® B 4300 G6 HR 30% Glass Filled BK 15116 PBT
Description: injection-molding grade with 30% glass-fibers; for rigid and dimensionally stable technical parts with increased requirements on hydrolysis resistance. For example automotive connectors..
Linear Mold Shrinkage, Transverse 0.013 cm/cm
0.013 in/in
375°C nozzle, 180°C tool; ISO 294-4
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac..
Copyright © lookpolymers.com All Rights Reserved