Polymer Property : Linear Mold Shrinkage, Transverse = 0.016 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.016 cm/cm
0.016 in/in
ASTM D955
NYCOA 5100 HS Heat Stabilized, Impact Modified Nylon 66 Resin
NYCOA 5100 HS is an impact modified, heat stabilized Nylon 66 resin used for injection molding. This material is specially formulated to provide improved flexibility and ductility vs standard Nylon ..
Linear Mold Shrinkage, Transverse 0.016 cm/cm

@Thickness 2.00 mm
0.016 in/in

@Thickness 0.0787 in
ISO 294-4
DuPont Performance Polymers Crastin® ST830FRUV NC010 PBT  (Unverified Data**)
Crastin® ST830FRUV NC010 is an unreinforced, Super Tough, flame retardant polybutylene terephthalate resin for injection molding. It contains a UV light stabilizer and is recognized as UL94V-0 at 0..
Linear Mold Shrinkage, Transverse 0.016 cm/cm
0.016 in/in
ASTM D955
LG Chemical LUPOL TE-5006K Thermoplastic Elastomer Alloy, Weather Resistant
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem
Linear Mold Shrinkage, Transverse 0.016 cm/cm

@Time 86400 sec
0.016 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRILOY UX98388 PPA
LNP LUBRILOY* UX98388 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.016 - 0.024 cm/cm

@Thickness 2.30 - 4.60 mm
0.016 - 0.024 in/in

@Thickness 0.0906 - 0.181 in
SABIC Method
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East)
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm

@Thickness 3.20 mm
0.016 - 0.018 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Xenoy® 6620 PBT+PC
PBT+PC, Unreinforced, impact modified thermoplastic alloy. Outstanding impact at low temperature
Linear Mold Shrinkage, Transverse 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
ISO DIS 294-4
Wellman Wellamid® 22LH-NBK4/WE1657 Unfilled Nylon 66
Description: Unfilled Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
ISO DIS 294-4
Wellman Wellamid® XT1482-WT1 High Impact Nylon 66
Description: High Impact Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
ISO DIS 294-4
Wellman Wellamid® XT1627-WBK2 High Impact, Weatherable Nylon 66
Description: High Impact, Weatherable Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.016 cm/cm
0.016 in/in
ISO 294-4 2577
DuPont Performance Polymers Crastin® S610SF BK851 Polybutylene Terephthalate (PBT)
Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin S610SF is an unreinforced low viscosity polybutylene terephthalate for injection molding. It has hig..
Linear Mold Shrinkage, Transverse 0.016 cm/cm
0.016 in/in
ISO 294-4 2577
DuPont Performance Polymers Crastin® S610SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)<
Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin S610SF is an unreinforced low viscosity polybutylene terephthalate for injection molding. It has hig..
Linear Mold Shrinkage, Transverse 0.016 cm/cm
0.016 in/in
ISO 294-4 2577
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)  (Unverified Data**)
Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri..
Linear Mold Shrinkage, Transverse 0.016 cm/cm
0.016 in/in
ISO 294-4 2577
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Transverse 0.016 cm/cm
0.016 in/in
Eurotec
Eurotec® Tecoform® PO20 GR25 NL HS POM, 25% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
Linear Mold Shrinkage, Transverse 0.016 cm/cm
0.016 in/in
ISO 294-4 2577
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc..
Linear Mold Shrinkage, Transverse 0.016 cm/cm

@Thickness 2.00 mm
0.016 in/in

@Thickness 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® 20NSP Nylon 66, Conditioned
Vydyne® 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin available in natural color. It is designed to crystallize rapidly in order to reduce cycle times and increase productivit..
Linear Mold Shrinkage, Transverse 0.016 cm/cm
0.016 in/in
ISO Data
BASF Ultraform N 2640 Z6 UNC POM
Ultraform N 2640 Z6 UNC is an elastomer-modified injection molding POM grade with excellent impact strength.
Linear Mold Shrinkage, Transverse 0.016 cm/cm

@Diameter 2.00 mm
0.016 in/in

@Diameter 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, Conditioned
Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..
Linear Mold Shrinkage, Transverse 0.016 cm/cm

@Diameter 2.00 mm
0.016 in/in

@Diameter 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM
Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..
Linear Mold Shrinkage, Transverse 0.016 cm/cm

@Thickness 2.00 mm
0.016 in/in

@Thickness 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® 47 Nylon 66, DAM
Vydyne® 47 Nylon resins are general purpose polyamide, impact modified grades. They are available in natural, black and heat stabilized for improved resistance to elevated temperatures. The heat st..
Linear Mold Shrinkage, Transverse 0.016 cm/cm

@Diameter 2.00 mm
0.016 in/in

@Diameter 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, Conditioned
Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra..
Linear Mold Shrinkage, Transverse 0.016 cm/cm

@Diameter 2.00 mm
0.016 in/in

@Diameter 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, Conditioned
Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4..
Linear Mold Shrinkage, Transverse 0.016 cm/cm

@Thickness 2.00 mm
0.016 in/in

@Thickness 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® 49 Nylon 66, DAM
Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp..
Linear Mold Shrinkage, Transverse 0.016 cm/cm

@Diameter 2.00 mm
0.016 in/in

@Diameter 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, Conditioned
Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
Linear Mold Shrinkage, Transverse 0.016 cm/cm

@Diameter 2.00 mm
0.016 in/in

@Diameter 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, Conditioned
Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista..
Linear Mold Shrinkage, Transverse 0.016 cm/cm

@Thickness 3.20 mm
0.016 in/in

@Thickness 0.126 in
Unitika EX-1030 PA6, Conditioned
High-impact nylonInformation provided by Unitika Ltd.