| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 400000 cP | 400000 cP | Melt Viscosity; SABIC Method |
|
SABIC Innovative Plastics Valox® 309 PBT
PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 3500-4500. Available in Natural (1001) only.
|
|||
| Viscosity | 400000 cP | 400000 cP | melt; SABIC Method |
|
SABIC Innovative Plastics Valox® EF4530 PBT (Asia Pacific)
Easy flow, 30% glass-reinforced, PBTP resin. Flame retardant.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Viscosity | 400000 cP | 400000 cP | A |
|
Shin-Etsu Silicones LIMSâ„¢ KE2001-40A/B Elastomer
Information Provided by Shin-Etsu Silicones of America, Inc.
|
|||
| Viscosity | 400000 cP | 400000 cP | B |
|
Shin-Etsu Silicones LIMSâ„¢ KE2001-40A/B Elastomer
Information Provided by Shin-Etsu Silicones of America, Inc.
|
|||
| Viscosity |
400000
cP @Temperature 25.0 °C |
400000
cP @Temperature 77.0 °F |
Dynamic |
|
Struktol VP 3695 Elastomer modified epoxy prepolymer
Applications: STRUKTOL POLYDIS 3695 is used where conventional epoxy systems are unable to satisfy the demands of for example contact adhesion or peel strength. Improvements in impact strength, flex..
|
|||
| Viscosity |
400000
cP @Shear Rate 1000 1/s, Temperature 240 °C |
400000
cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
|
DSM Akulon® F130 PA6
Film Extrusion, Medium Viscosity
|
|||
| Viscosity |
400000
cP @Shear Rate 1000 1/s, Temperature 240 °C |
400000
cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
|
DSM Akulon® F130-C PA6
Film Extrusion, Medium Viscosity, Lubricated
|
|||
| Viscosity |
400000
cP @Shear Rate 1000 1/s, Temperature 240 °C |
400000
cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
|
DSM Akulon® F130-C2 PA6
Medium Viscosity, Film Extrusion, Lubricated
|
|||
| Viscosity |
400000
cP @Shear Rate 1000 1/s, Temperature 240 °C |
400000
cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
|
DSM Akulon® F130-E1 PA6
Medium Viscosity, Nucleated, Lubricated, Film Extrusion
|
|||
| Viscosity |
400000
cP @Shear Rate 1000 1/s, Temperature 240 °C |
400000
cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
|
DSM Akulon® F130-E5 PA6
Medium Viscosity, Nucleated, Lubricated, Film Extrusion, Antiblock
|
|||
| Viscosity |
400000
cP @Shear Rate 1000 1/s, Temperature 240 °C |
400000
cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
|
DSM Akulon® F132-C1 PA6
Film Extrusion, High Viscosity, Lubricated
|
|||
| Viscosity |
400000
cP @Shear Rate 1000 1/s, Temperature 240 °C |
400000
cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
|
DSM Akulon® F132-E1 PA6
Medium/High Viscosity, Nucleated, Lubricated, Film Extrusion
|
|||
| Viscosity |
400000
cP @Shear Rate 1000 1/s, Temperature 240 °C |
400000
cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
|
DSM Akulon® F132-E2 PA6
High Viscosity, Nucleated, Lubricated, Film Extrusion
|
|||
| Viscosity |
400000
cP @Shear Rate 1000 1/s, Temperature 240 °C |
400000
cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
|
DSM Akulon® F136 PA6
Very High Viscosity, Film Extrusion
|
|||
| Viscosity |
400000
cP @Shear Rate 1000 1/s, Temperature 260 °C |
400000
cP @Shear Rate 1000 1/s, Temperature 500 °F |
|
|
DSM Akulon® F136 PA6
Very High Viscosity, Film Extrusion
|
|||
| Viscosity |
400000
cP @Shear Rate 1000 1/s, Temperature 240 °C |
400000
cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
|
DSM Akulon® F136-C PA6
Film Extrusion, Very High Viscosity, Lubricated
|
|||
| Viscosity |
400000
cP @Shear Rate 1000 1/s, Temperature 280 °C |
400000
cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
|
DSM Akulon® F136-C PA6
Film Extrusion, Very High Viscosity, Lubricated
|
|||
| Viscosity |
400000
cP @Shear Rate 1000 1/s, Temperature 260 °C |
400000
cP @Shear Rate 1000 1/s, Temperature 500 °F |
|
|
DSM Akulon® F136-C1 PA6
Very High Viscosity, Film Extrusion, Lubricated
|
|||
| Viscosity |
400000
cP @Shear Rate 1000 1/s, Temperature 240 °C |
400000
cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
|
DSM Akulon® F136-E1 PA6
Very High Viscosity, Lubricated, Nucleated, Film Extrusion
|
|||
| Viscosity |
400000
cP @Shear Rate 1000 1/s, Temperature 260 °C |
400000
cP @Shear Rate 1000 1/s, Temperature 500 °F |
|
|
DSM Akulon® F136-E1 PA6
Very High Viscosity, Lubricated, Nucleated, Film Extrusion
|
|||
| Viscosity |
400000
cP @Shear Rate 1000 1/s, Temperature 280 °C |
400000
cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
|
DSM Akulon® F136-E1 PA6
Very High Viscosity, Lubricated, Nucleated, Film Extrusion
|
|||
| Viscosity |
400000
cP @Shear Rate 0.100 1/s, Temperature 280 °C |
400000
cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
|
DSM Akulon® F128 PA6
Film Extrusion, Medium Viscosity
|
|||
| Viscosity | >= 400000 cP | >= 400000 cP | 0.5 rpm, uncured |
|
Atom Adhesives AA-BOND G298 Epoxy Adhesive
AA-BOND G298 is a two component, gold-filled, electrically and thermally conductive epoxy designed for hybrid microelectronic and semiconductor packaging.Appearance: Resin: Brown, Hardener: Dark Bro..
|
|||
| Viscosity |
400000
-
800000
cP @Shear Rate 100 1/s, Temperature 232 °C |
400000
-
800000
cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
|
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
|
|||
| Viscosity |
400000
-
800000
cP @Shear Rate 100 1/s, Temperature 232 °C |
400000
-
800000
cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
|
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
|
|||
| Viscosity | 400000 cP | 400000 cP | Mixed |
|
Armstrong A-1/E Epoxy Adhesive
A brown epoxy paste formulated with enhanced wetting capabilities to hard rubbers and rigid thermoplastics. Has low outgassing characteristics at temperatures below 250°FInformation provided by El..
|
|||
| Viscosity |
400000
cP @Shear Rate 300 1/s, Temperature 190 °C |
400000
cP @Shear Rate 300 1/s, Temperature 374 °F |
ASTM D3835 |
|
Advanced Polymer Alloys Alcryn® 4660 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
|
|||
| Viscosity |
400000
-
800000
cP @Shear Rate 100 1/s, Temperature 232 °C |
400000
-
800000
cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
|
Arkema Group KYNAR® 711 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan..
|
|||
| Viscosity |
400000
-
1.20e+6
cP @Shear Rate 100 1/s, Temperature 232 °C |
400000
-
1.20e+6
cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
|
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
|
|||