Polymer Property : Viscosity = 800000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 600000 - 800000 cP

@Temperature 25.0 °C
600000 - 800000 cP

@Temperature 77.0 °F
Uncured
Permabond ES578 Epoxy Resin
PERMABOND® ES578 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces, ceramics as well as composite materials. ES578 provides excellent thermal conductivity and bon..
Viscosity 8000 - 800000 cP

@Temperature 230 - 270 °C
8000 - 800000 cP

@Temperature 446 - 518 °F
Average value: 187000 cP Grade Count:2
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Viscosity 8000 - 800000 cP

@Shear Rate 1.00 - 100000 1/s
8000 - 800000 cP

@Shear Rate 1.00 - 100000 1/s
Average value: 187000 cP Grade Count:2
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Viscosity 500000 - 800000 cP
500000 - 800000 cP
Lord Adhesives 310 High Strength SMC, FRP and General Purpose Epoxy Adhesive
Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh..
Viscosity 400000 - 800000 cP

@Shear Rate 100 1/s,
Temperature 232 °C
400000 - 800000 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Viscosity 400000 - 800000 cP

@Shear Rate 100 1/s,
Temperature 232 °C
400000 - 800000 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Viscosity 400000 - 800000 cP

@Shear Rate 100 1/s,
Temperature 232 °C
400000 - 800000 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR® 711 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan..
Viscosity 500000 - 800000 cP

@Shear Rate 100 1/s,
Temperature 232 °C
500000 - 800000 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR® 9000 HD Polyvinylidene Fluoride - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Viscosity 300000 - 800000 cP
300000 - 800000 cP
Part B
Master Bond EP21TDC-2LO Two component, highly flexibilized epoxy resin compound
Product Description: Master Bond Polymer System EP21TDC-2LO is a two component, highly flexible epoxy resin compound for high performance bonding, sealing, coating, and encapsulation. It is formulat..
Viscosity 500000 - 800000 cP

@Shear Rate 100 1/s,
Temperature 232 °C
500000 - 800000 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt Viscosity; ASTM D3835
Arkema Group KYNAR FLEX® 2850 PC Polyvinylidene Fluoride Spray Coating Powder
Electrostatic sprayInformation provided by Arkema Inc.