Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 0.370 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.370 J/cm
<br>@Temperature -30.0 °C
0.693 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Cycolac® MG34LGHF ABS
Low gloss, high flow ABS for unpainted interior applications.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 0.370 J/cm
<br>@Temperature -40.0 °C
0.693 ft-lb/in
<br>@Temperature -40.0 °F
ASTM D 256
SABIC Innovative Plastics Cycolac® X17 ABS
Automotive: Very high heat resistance with high strength and modulus. UL94 HB rated.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 0.370 J/cm
<br>@Thickness 4.00 mm,<br> Temperature -20.0 °C
0.693 ft-lb/in
<br>@Thickness 0.157 in,<br> Temperature -4.00 °F
ISO 180
Premix Thermoplastics PRE-ELEC® PP 1375
PRE-ELEC PP 1375 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..
Izod Impact, Notched 0.370 J/cm
<br>@Temperature -30.0 °C
0.693 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® ML7677A PC (Asia Pacific)
Commercial grade for Polycarbonate in only nature color. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm.This data was supplied by SABIC-IP for the Asia Pacific reg..
Izod Impact, Notched 0.370 J/cm
<br>@Thickness 6.35 mm,<br> Temperature 23.0 °C
0.693 ft-lb/in
<br>@Thickness 0.250 in,<br> Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Fittings M1000 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Izod Impact, Notched 0.370 J/cm
<br>@Thickness 6.35 mm,<br> Temperature 23.0 °C
0.693 ft-lb/in
<br>@Thickness 0.250 in,<br> Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Fittings M1005 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Izod Impact, Notched 0.370 J/cm
<br>@Temperature -40.0 °C
0.693 ft-lb/in
<br>@Temperature -40.0 °F
ASTM D256
Eastman Eastar GN002 Copolyester, Natural &nbsp;(discontinued **)
Eastar GN002 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN002 copolyester will not crystallize and thus offers wider processing latitude tha..
Izod Impact, Notched 0.370 J/cm
<br>@Temperature -40.0 °C
0.693 ft-lb/in
<br>@Temperature -40.0 °F
ASTM D256
Eastman Eastar GN005 Copolyester, Natural &nbsp;(discontinued **)
Eastar GN005 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN005 copolyester will not crystallize and thus offers wider processing latitude tha..
Izod Impact, Notched 0.370 J/cm
<br>@Thickness 4.00 mm,<br> Temperature 23.0 °C
0.693 ft-lb/in
<br>@Thickness 0.157 in,<br> Temperature 73.4 °F
ISO 180
Premix Thermoplastics PRE-ELEC® PPE 1462 &nbsp;(discontinued **)
PRE-ELEC PPE 1462 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric..
Izod Impact, Notched 0.370 J/cm
<br>@Temperature 23.0 °C
0.693 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer
Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 0.370 J/cm
<br>@Thickness 6.35 mm,<br> Temperature 23.0 °C
0.693 ft-lb/in
<br>@Thickness 0.250 in,<br> Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Fittings M1012 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Izod Impact, Notched 0.370 J/cm
<br>@Temperature 23.0 °C
0.693 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Ultem 1100FV PEI
Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th..
Izod Impact, Notched 0.370 J/cm
<br>@Temperature -30.0 °C
0.693 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Ultem 1100FV PEI
Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th..
Izod Impact, Notched 0.370 J/cm
<br>@Temperature 23.0 °C
0.693 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Ultem 1100FV PEI (Asia Pacific)
Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th..
Izod Impact, Notched 0.370 J/cm
<br>@Temperature -30.0 °C
0.693 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Ultem 1100FV PEI (Asia Pacific)
Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th..
Izod Impact, Notched 0.370 J/cm
<br>@Temperature 23.0 °C
0.693 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Ultem 1100FV PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th..
Izod Impact, Notched 0.370 J/cm
<br>@Temperature -30.0 °C
0.693 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Ultem 1100FV PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th..
Izod Impact, Notched 0.370 J/cm
<br>@Temperature -30.0 °C
0.693 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS
Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e..
Izod Impact, Notched 0.370 J/cm
<br>@Temperature -30.0 °C
0.693 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Asia Pacific)
Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e..
Izod Impact, Notched 0.370 J/cm
<br>@Temperature -30.0 °C
0.693 ft-lb/in
<br>@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Europe-Africa-Middle East)
Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e..
Izod Impact, Notched 0.370 J/cm
<br>@Temperature -20.0 °C
0.693 ft-lb/in
<br>@Temperature -4.00 °F
ASTM D256
Total PPC 4820WZ Polypropylene, Impact Copolymer
TOTAL Petrochemicals Polypropylene 4820WZ is a nucleated impact copolymer with a Melt Flow index of 35 g/10 min.TOTAL Polypropylene 4820WZ is characterized by improved stiffness, creep resistance, h..
Izod Impact, Notched 0.370 J/cm
<br>@Temperature -40.0 °C
0.693 ft-lb/in
<br>@Temperature -40.0 °F
ASTM D256
Eastman Drystar 0113 Copolyester
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..
Izod Impact, Notched 0.370 J/cm
<br>@Temperature -40.0 °C
0.693 ft-lb/in
<br>@Temperature -40.0 °F
ASTM D256
Eastman Drystar 0601 Copolyester, Injection Molded
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..
Izod Impact, Notched 0.370 J/cm
<br>@Temperature -40.0 °C
0.693 ft-lb/in
<br>@Temperature -40.0 °F
ASTM D256
Eastman Eastar MN210 Copolyester, Natural
Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates.Applications/UsesMedical
Izod Impact, Notched 0.370 J/cm
<br>@Temperature -40.0 °C
0.693 ft-lb/in
<br>@Temperature -40.0 °F
ASTM D256
Eastman Eastar MN211 Copolyester, Natural
Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. MN211 contains a mold release.Application..
Izod Impact, Notched 0.370 J/cm
<br>@Temperature -40.0 °C
0.693 ft-lb/in
<br>@Temperature -40.0 °F
ASTM D256
Eastman Eastman 1223 Copolyester
Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card..
Izod Impact, Notched 0.370 J/cm
<br>@Temperature -40.0 °C
0.693 ft-lb/in
<br>@Temperature -40.0 °F
ASTM D256
Eastman GSP01 Copolyester for Film and Sheet Extrusion
Applications:Consumer e-packaging trayElectronic packagingElectrostatic dissipative trayProduct Description: GSP01 is a clear, amorphous material. Because of its clarity, toughness and good melt s..
Izod Impact, Notched 0.370 J/cm
<br>@Temperature -20.0 °C
0.693 ft-lb/in
<br>@Temperature -4.00 °F
ASTM D256
Braskem CP 741 Extrusion Polypropylene Heterophasic Copolymer
Sheet extrusion.Information provided by Braskem.
Izod Impact, Notched 0.370 J/cm
<br>@Temperature -20.0 °C
0.693 ft-lb/in
<br>@Temperature -4.00 °F
ASTM-D256
Braskem CP 743 HECO Polypropylene Heterophasic Copolymer
CP 743 is a low melt flow rate heterophasic copolymer. It has broad molecular weight distribution and a general purpose additive package. CP 743 presents high melt strength, good processability, and..