| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Fittings M1005 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | ASTM D955 |
| Spiral Flow | 63.5 cm | 25.0 in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 81 | 81 | ASTM D2240 |
| Tensile Strength, Yield | 49.6 MPa | 7190 psi | Type I, 51 mm/min; ASTM D638 |
| Tensile Modulus | 3.03 GPa | 439 ksi | Type I, 51 mm/min; ASTM D638 |
| Flexural Strength | 91.0 MPa | 13200 psi | ASTM D790 |
| Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
| Izod Impact, Notched | 0.370 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.693 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| 0.530 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.993 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 72.8 °C @Thickness 6.35 mm |
163 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 72.2 °C @Thickness 6.35 mm |
162 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 199 - 210 °C | 390 - 410 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | Medium Flow | |
| Forms | Pellets | |
| Generic Material | PVC, Rigid | |
| Generic Name | Polyvinyl Chloride, Rigid (PVC, Rigid) | |
| Processing Method | Injection Molding | |
| PVC Cell Classification | 12454 | ASTM D1784 |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Fittings |