Polymer Property : Flexural Strength = 97.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Strength 97.0 MPa
14100 psi
Plastcom SLOVAMID 66 LI PA66, improved strength
FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe..
Flexural Strength 97.0 MPa
14100 psi
Poco Graphite ACF-10Q Industrial Grade Graphite
POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr..
Flexural Strength 97.0 MPa
14100 psi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP IFL21 PA6.12
LNP LUBRICOMP* IFL21 is a compound based on Nylon 6/12 resin containing 5% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant.
Flexural Strength 97.0 MPa
14100 psi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP OL004 PPS - Linear
LNP* LUBRICOMP* OL004 is a compound based on PPS - Linear resin containing 20% PTFE. Added features of this grade include: Wear Resistant.
Flexural Strength 97.0 MPa
14100 psi
ASTM D790
Stratasys® Polycarbonate
A true industrial thermoplastic, PC (polycarbonate) is widely used in automotive, aerospace, medical and many other applications. PC offers accuracy, durability and stability, creating strong parts ..
Flexural Strength 97.0 MPa
14100 psi
2.0 mm/min; ISO 178
Styron CALIBREâ„¢ 200-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 200-10 Series are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance, heat distor..
Flexural Strength 97.0 MPa
14100 psi
2.0 mm/min; ISO 178
Styron CALIBREâ„¢ 200-14 Polycarbonate Resin
Overview: CALIBREâ„¢ 200-14 polycarbonate resin is a natural, FDA compliant, 14 melt flow rate general purpose polycarbonate resin with no mold release or UV stabilizer.Govt. and Industry Standar..
Flexural Strength 97.0 MPa
14100 psi
2.0 mm/min; ISO 178
Styron CALIBREâ„¢ 201-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 201-10 is produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. It provides excellent impact resistance, heat distortion resi..
Flexural Strength 97.0 MPa
14100 psi
2.0 mm/min; ISO 178
Styron CALIBREâ„¢ 201-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 201-15 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc..
Flexural Strength 97.0 MPa
14100 psi
2.0 mm/min; ISO 178
Styron CALIBREâ„¢ 201-22 Polycarbonate Resin
Overview: CALIBREâ„¢ 201-22 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc..
Flexural Strength 97.0 MPa
14100 psi
2.0 mm/min; ISO 178
Styron CALIBREâ„¢ 201-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 201-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance..
Flexural Strength 97.0 MPa
14100 psi
2.0 mm/min; ISO 178
Styron CALIBREâ„¢ 203-22 Polycarbonate Resin
Overview: CALIBREâ„¢ 200-22 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc..
Flexural Strength 97.0 MPa
14100 psi
2.0 mm/min; ISO 178
Styron CALIBREâ„¢ 301EP-22 Polycarbonate Resin
Overview: CALIBREâ„¢ 300EP-22 Series are polycarbonate resins that offer exceptional impact resistance, heat distortion resistance and optical clarity for injection molding applications. Their hi..
Flexural Strength 97.0 MPa
14100 psi
2.0 mm/min; ISO 178
Styron CALIBREâ„¢ 302-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-10 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet appli..
Flexural Strength 97.0 MPa
14100 psi
2.0 mm/min; ISO 178
Styron CALIBREâ„¢ 303-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-115 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity. The CALIBREâ„¢ 300-10 series products are available in 4 ..
Flexural Strength 97.0 MPa
14100 psi
2.0 mm/min; ISO 178
Styron CALIBREâ„¢ 303-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 300-6 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet applic..
Flexural Strength 97.0 MPa
14100 psi
3 points, 2 mm/min; ISO 178
Styron TYRILâ„¢ 875 SAN Resin
Overview: TYRIL Styrene-actylonitrile (SAN) resins are designed by Styron to offer superior chemical resistance, strength, hardness and dimensional stability in a broad range of product applications..
Flexural Strength 97.0 MPa
14100 psi
ASTM D790
Lubrizol Isoplast® 2531 Engineering Thermoplastic Polyurethane Resin for Medical Applications
Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Flexural Strength 97.0 MPa
14100 psi
Cosmic Plastics 6220 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Flexural Strength 97.0 MPa
14100 psi
Cosmic Plastics 6220F Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Flexural Strength 97.0 MPa
14100 psi
Cosmic Plastics K31 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Flexural Strength 97.0 MPa
14100 psi
Cosmic Plastics D72 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Flexural Strength 97.0 MPa
14100 psi
2 mm/min; ISO 178
Covestro Makrolon® 2405 MAS048 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Flexural Strength 97.0 MPa
14100 psi
2 mm/min; ISO 178
Covestro Makrolon® 2652 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..
Flexural Strength 97.0 MPa
14100 psi
2 mm/min; ISO 178
Covestro Makrolon® 2805 MAS145 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Flexural Strength 97.0 MPa
14100 psi
2 mm/min; ISO 178
Covestro Makrolon® 2805 MAS152 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
Flexural Strength 97.0 MPa
14100 psi
Du-Co Ceramics DC-65 Cordierite
Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company.
Flexural Strength 97.0 MPa
14100 psi
ASTM D790
A. Schulman ComAlloy Comtuf® 520 Polycarbonate/Styrenic Alloy
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc..
Flexural Strength 97.0 MPa
14100 psi
ASTM D790
Styrolution NAS® 21 Acrylic Copolymer
Features:Sparkling clarity Scratch resistant Can be blended with K-Resin at any level to modify flexibility, surface hardness, heat distortion temperatures, etc. Styrenic processing advantages Gamma..
Flexural Strength 97.0 MPa
14100 psi
Cosmic Plastics D33 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.