Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 2.09 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.440 - 0.440 J/cm²

@Temperature -30.0 - -30.0 °C
2.09 - 2.09 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.440 J/cm² Grade Count:1
Overview of materials for Acetal Copolymer, Steel Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of..
Charpy Impact, Notched 0.440 J/cm²

@Temperature -30.0 °C
2.09 ft-lb/in²

@Temperature -22.0 °F
Eastman Tenite 383A-08 Cellulose Acetate Propionate  (discontinued **)
8% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
Charpy Impact, Notched 0.440 J/cm²

@Temperature -30.0 °C
2.09 ft-lb/in²

@Temperature -22.0 °F
Eastman Tenite 371A-08 Cellulose Acetate Propionate  (discontinued **)
8% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
Charpy Impact, Notched 0.440 - 0.550 J/cm²

@Temperature -30.0 - -30.0 °C
2.09 - 2.62 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.495 J/cm² Grade Count:2
Overview of materials for Nylon 11 with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are includ..
Charpy Impact, Notched 0.440 J/cm²

@Temperature 23.0 °C
2.09 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1e
Aardvark Polymers AARTEL® 100 D/S Rotational Molding Resin
Aartel 100SD is a new conductive grade developed to dissipate electricity in fuel handling systems. Aartel 100SD maintains all o the excellent properties of our general purpose acetal, has a volume ..
Charpy Impact, Notched 0.440 J/cm²

@Temperature -23.0 °C
2.09 ft-lb/in²

@Temperature -9.40 °F
DIN 53453
Global PP-3342-M Polypropylene Random Copolymer
Description-medium stiffness, low melting temperatures, very good for seal Applications-housewares, cookwareInformation provided by Global Polymers Corporation.
Charpy Impact, Notched 0.440 J/cm²
2.09 ft-lb/in²
ASTM D256
Plenco 6401 Phenolic, Briquette, Transfer Molded
PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco.
Charpy Impact, Notched 0.440 J/cm²

@Temperature -40.0 °C
2.09 ft-lb/in²

@Temperature -40.0 °F
ISO R179
Arkema Group ORGASOL® 2002 D Nat 1 Polyamide 12, Food Contact Approved
Information provided by Arkema Group
Charpy Impact, Notched 0.440 J/cm²

@Temperature -30.0 °C
2.09 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® AESN P20 TL Nylon 12, Flexible Grade (Dry)
Designation ISO 1874-PA12-P,EHL,22-005Flexible grade for overmolding. Available colors: natural and white. Light and heat stabilized. No lubricant.Flexibility. Very good ability to overmold Pebax an..
Charpy Impact, Notched 0.440 J/cm²
2.09 ft-lb/in²
Arkema Group Rilsan® AMN G8 TLD Nylon 12, Graphite Filled (Conditioned)
Designation ISO 1874-PA12,MHLS,14-010,CD05Rigid grade with graphite filler for injection molding. Available colors: steel gray. Light and heat stabilized. Mold-release agent.Low friction coefficient..
Charpy Impact, Notched 0.440 J/cm²
2.09 ft-lb/in²
Arkema Group Rilsan® ARVO 950 TLD Nylon 12, Rotomolding Grade (Dry)
Designation ISO 1874-PA12,RHLR,16-010Grade for rotomolding. Available color: natural. Light and heat stabilized. Mold-release agent.Easy to be processed in the same conditions as polyethylene. High ..
Charpy Impact, Notched 0.440 J/cm²
2.09 ft-lb/in²
Arkema Group Rilsan® AUM 50 NOIR T6LD Nylon 12, 50% Glass Bead Filled (Conditioned)
Designation ISO 1874-PA12,MHLR,16-020,GB50Rigid grad with glass beads filler (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agents. Mold-release agent.Goo..
Charpy Impact, Notched 0.440 J/cm²

@Temperature -30.0 °C
2.09 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® BESN F15 TL Nylon 11, Flexible Tubing Grade (Dry)
Designation ISO 1874-PA11-P,EHL,16-001High flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High burst pressure and impact strength..
Charpy Impact, Notched 0.440 J/cm²

@Temperature -30.0 °C
2.09 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® BZM 8 NOIR TL Nylon 11, 8% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA11,MHL,18-020,GF8Rigid grade with glass fiber (8%) filler for injection molding. Available color: black. Light and heat stabilized.Rigidity. Outstanding compromise between goo..
Charpy Impact, Notched 0.440 J/cm²
2.09 ft-lb/in²
ISO 179
BASF Ultramid® B3WGM24 HPX BK 2320 30% Glass/Mineral Filled PA6 (Dry)
Description: Ultramid B3WGM24 HPX BK23210 is a very high productivity, 30% glass/mineral reinforced heat stabilized injection molding PA6 grade for components that require medium rigidity, excellent..
Charpy Impact, Notched 0.440 J/cm²

@Temperature -30.0 °C
2.09 ft-lb/in²

@Temperature -22.0 °F
ISO data
BASF Capron® 8203C HS Blend Nylon 6 (Dry)  (discontinued **)
Capron 8203C HS Blend is a heat stabilized, high viscosity nylon 6 extrusion compound possessing a modified crystalline structure for increased strength, stiffness and heat distortion temperature. ..
Charpy Impact, Notched 0.440 J/cm²
2.09 ft-lb/in²
ISO 179
Solvay Specialty Polymers Ixef® 2060 Polyarylamide (PARA)  (discontinued **)
Ixef 2060 is a 55% reinforced, general purpose polyarylamide compound. This compound exhibits improved vibration resistance, low warpage, and excellent surface finish. This grade has excellent prope..
Copyright © lookpolymers.com All Rights Reserved