Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Global PP-3342-M Polypropylene Random Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Global Polymers Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global PP-3342-M Polypropylene Random Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description-medium stiffness, low melting temperatures, very good for seal Applications-housewares, cookwareInformation provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
L; ASTM D1238
Mechanical Properties Metric English Comments
Ball Indentation Hardness 64.0 MPa
9280 psi
DIN 53456
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Shear Modulus 0.580 GPa
84.1 ksi
DIN 53457
Charpy Impact, Notched 0.440 J/cm²

@Temperature -23.0 °C
2.09 ft-lb/in²

@Temperature -9.40 °F
DIN 53453
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
Unannealed; ASTM D648