Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.518 J/cm | 0.970 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.518 J/cm | 0.970 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.518 J/cm | 0.970 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.518 J/cm | 0.970 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.518 J/cm | 0.970 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.518 J/cm | 0.970 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.518 J/cm | 0.970 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0334C20L1 Calcium Reinforced |
|||
Izod Impact, Notched | 0.518 - 2.14 J/cm | 0.970 - 4.00 ft-lb/in | Average value: 1.24 J/cm Grade Count:30 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |