| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 0.320 - 2.14 J/cm | 0.600 - 4.01 ft-lb/in | Average value: 0.748 J/cm Grade Count:26 |
|
Overview of materials for Polyphthalamide (PPA), Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of ..
|
|||
| Izod Impact, Notched | 0.107 - 2.14 J/cm | 0.200 - 4.00 ft-lb/in | Average value: 0.596 J/cm Grade Count:13 |
|
Overview of materials for Epoxy Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat..
|
|||
| Izod Impact, Notched | 0.160 - 2.14 J/cm | 0.300 - 4.00 ft-lb/in | Average value: 1.57 J/cm Grade Count:4 |
|
Overview of materials for Polyphenylene Ether, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Mineral Filled". Each property range of values reported is minimum and maximum valu..
|
|||
| Izod Impact, Notched | 0.267 - 2.14 J/cm | 0.500 - 4.01 ft-lb/in | Average value: 0.801 J/cm Grade Count:67 |
|
Overview of materials for Polycarbonate, Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val..
|
|||
| Izod Impact, Notched | 0.640 - 2.14 J/cm | 1.20 - 4.00 ft-lb/in | Average value: 1.54 J/cm Grade Count:30 |
|
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
|
|||
| Izod Impact, Notched | 0.427 - 2.14 J/cm | 0.800 - 4.01 ft-lb/in | Average value: 0.972 J/cm Grade Count:84 |
|
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values..
|
|||
| Izod Impact, Notched | 0.374 - 2.14 J/cm | 0.700 - 4.01 ft-lb/in | Average value: 0.780 J/cm Grade Count:10 |
|
Overview of materials for Nylon 66, Mineral Filled, NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, NCG Fiber Filled". Each property range of values reported is minimum and maxim..
|
|||
| Izod Impact, Notched | 0.961 - 2.14 J/cm | 1.80 - 4.00 ft-lb/in | Average value: 1.40 J/cm Grade Count:7 |
|
Overview of materials for Nylon 11 + Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp..
|
|||
| Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | ASTM D256 |
|
Mar-Bal MB2000-8 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
|
|||
| Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | ASTM D256 |
|
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | ASTM D256 |
|
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli..
|
|||
| Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | ASTM D256 |
|
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | ASTM D256 |
|
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Izod Impact, Notched | 1.60 - 2.14 J/cm | 3.00 - 4.00 ft-lb/in | |
|
Bulk Molding Compounds BMC 1403 Electrical Grade
BMC 1403 is one of the most useful general-purpose electrical grade materials available on the market. Competitive against phenolic, melamine, and urea materials for electrical applications. Easy mo..
|
|||
| Izod Impact, Notched | 1.60 - 2.14 J/cm | 3.00 - 4.00 ft-lb/in | |
|
Bulk Molding Compounds BMC 2270 Mineral Filled, Glass Reinforced Polyester
BMC 2270 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a general purpose material with medium impact strength a..
|
|||
| Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
|
Bulk Molding Compounds BMC 3001H Mineral Filled Alkyd
BMC 3001H molding compound is a mineral filled, glass-fiber reinforced alkyd compound suitable for compression and transfer molding. Because of its soft flow, it is also used extensively in cold spu..
|
|||
| Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
|
Bulk Molding Compounds BMC 605L Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 605L molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda..
|
|||
| Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
|
Bulk Molding Compounds BMC 610 - SP Mineral Filled, Glass Reinforced Polyester Compound, with UV Stabilizer
BMC 610 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is set a part form other medium impact el..
|
|||
| Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
|
Bulk Molding Compounds BMC 901 Encapsulating Grade Molding Compound
BMC 901 is an encapsulation grade, soft flow material. As with all other BMCI compounds, this series can be supplied in logs, slugs or bulk.Typical applications are electrical coil encapsulations an..
|
|||
| Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | ASTM D256 |
|
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
|
|||
| Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | ASTM D256 |
|
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, ..
|
|||
| Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
|
Bulk Molding Compounds BMC 1050 Thermoset Polyester
BMC 1050 is a cosmetic, appliance grade material with superior heat stability. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical applications are toaster e..
|
|||
| Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
|
Bulk Molding Compounds BMC 1901 Mineral Filled Alkyd
BMC 1901 molding compound is a mineral filled, glass-fiber-reinforced alkyd compound suitable for compression transfer molding. It is a general purpose with medium impact strength and good overall e..
|
|||
| Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
|
Bulk Molding Compounds BMC 200 Thermoset Polyester, Electrical Grade
BMC 200 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, bobbins, electrical conne..
|
|||
| Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
|
Bulk Molding Compounds BMC 2201 Mineral Filled Alkyd
BMC 2201 molding compound is a mineral filled, glass-fiber-and nylon-floc reinforced alkyd compound suitable for compression and transfer molding. It was developed for applications requiring better ..
|
|||
| Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
|
Bulk Molding Compounds BMC 2274 Mineral Filled, Glass Reinforced Polyester
BMC 2274 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression transfer and stuffer injection molding. It is a general-purpose material with medium..
|
|||
| Izod Impact, Notched | 0.214 - 2.14 J/cm | 0.400 - 4.00 ft-lb/in | Average value: 0.673 J/cm Grade Count:190 |
|
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..
|
|||
| Izod Impact, Notched |
1.07
-
2.14
J/cm <br>@Temperature 23.0 °C
|
2.00
-
4.01
ft-lb/in <br>@Temperature 73.4 °F
|
ASTM D256 |
|
Kleerdex Kydex® 160 Acrylic/PVC Thermoplastic Sheet
(discontinued **)
Class I/A rated thermoplastic sheetApplications: Interior ductwork and chutes, laboratory hoods, shower/tub shrouds, acoustical applications, decorative ceilings, abuse resistant surfacing for count..
|
|||
| Izod Impact, Notched | 0.518 - 2.14 J/cm | 0.970 - 4.00 ft-lb/in | Average value: 1.24 J/cm Grade Count:30 |
|
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and..
|
|||
| Izod Impact, Notched | 0.320 - 2.14 J/cm | 0.600 - 4.00 ft-lb/in | Average value: 0.644 J/cm Grade Count:22 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..
|
|||