Polymer Property : Izod Impact, Notched = 21.9 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 11.7 - 11.7 J/cm

@Temperature -40.0 - -40.0 °C
21.9 - 21.9 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 11.7 J/cm Grade Count:1
Overview of materials for PVC, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW..
Izod Impact, Notched 11.7 - 11.7 J/cm

@Thickness 3.18 - 3.18 mm
21.9 - 21.9 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 11.7 J/cm Grade Count:1
Overview of materials for PVC, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW..
Izod Impact, Notched 1.07 - 11.7 J/cm

@Temperature -40.0 - 10.0 °C
2.00 - 21.9 ft-lb/in

@Temperature -40.0 - 50.0 °F
Average value: 4.00 J/cm Grade Count:7
Overview of materials for PVC, High Impact
This property data is a summary of similar materials in the MatWeb database for the category "PVC, High Impact". Each property range of values reported is minimum and maximum values of appropriate M..
Izod Impact, Notched 1.07 - 11.7 J/cm

@Thickness 3.18 - 3.18 mm
2.00 - 21.9 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 4.00 J/cm Grade Count:7
Overview of materials for PVC, High Impact
This property data is a summary of similar materials in the MatWeb database for the category "PVC, High Impact". Each property range of values reported is minimum and maximum values of appropriate M..
Izod Impact, Notched 0.267 - 11.7 J/cm

@Temperature -40.0 - 10.0 °C
0.500 - 21.9 ft-lb/in

@Temperature -40.0 - 50.0 °F
Average value: 2.37 J/cm Grade Count:56
Overview of materials for PVC, Rigid Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M..
Izod Impact, Notched 0.267 - 11.7 J/cm

@Thickness 3.18 - 3.18 mm
0.500 - 21.9 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 2.37 J/cm Grade Count:56
Overview of materials for PVC, Rigid Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M..