Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched (ISO) = 4.76 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ISO 180
Premix Premi-Glas® 1266 (Injection Compression Molded) Glass Reinforced TMC
Description: Premi-Glas® 1266 is a glass reinforced thermoset molding compound designed for automotive under the hood applications. Key features and benefits: Designed for Injection or Injection/Co..
Izod Impact, Unnotched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ISO 180
Premix Premi-Glas® 1268 Fiberglass Reinforced Thermoset Thick Molding Compound
Premi-Glas® 1268 is a fiberglass reinforced thermoset thick molding compound for composite power train applications such as valve covers and timing gear covers.Key features and benefits are:Ideal f..
Izod Impact, Unnotched (ISO) 10.0 kJ/m²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Faradex AS0029 ABS (Europe-Africa-Middle East)
LNP* Faradex* AS-1002 FR is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Stainless Steel Fiber. Added features of this material include: Flame Retardant, EM..
Izod Impact, Unnotched (ISO) 10.0 kJ/m²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Konduit MT00EL PP
LNP* Konduit* MT00EL is a Polypropylene base resin with thermal fillers. Characteristics of this grade are Thermal Conductivity and it is Low Extraactible.This data was supplied by SABIC-IP for th..
Izod Impact, Unnotched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP AFP26 ABS (Europe-Africa-Middle East)
LNP* Lubricomp* AFP26 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, PTFE, Silicone.
Izod Impact, Unnotched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP BX05029 SAN (Europe-Africa-Middle East)
LNP* Lubricomp* BX05029 is a compound based on Styrene Acrylonitrile resin containing Mineral, Graphite.
Izod Impact, Unnotched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP CG006 PS (Europe-Africa-Middle East)
LNP* Lubricomp* CG006 is a compound based on Polystyrene resin containing Graphite.
Izod Impact, Unnotched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP CGI11 PS (Europe-Africa-Middle East)
LNP * Lubricomp* CGI11 is a compound based on Polystyrene resin containing Graphite. Added features include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 10.0 - 33.0 kJ/m²
4.76 - 15.7 ft-lb/in²
Average value: 17.2 kJ/m² Grade Count:6
Overview of materials for Cyclo Olefin Polymer
This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria..
Izod Impact, Unnotched (ISO) 10.0 - 95.0 kJ/m²
4.76 - 45.2 ft-lb/in²
Average value: 47.8 kJ/m² Grade Count:19
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Izod Impact, Unnotched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ASTM D256
Mitsui APELâ„¢ APL5014DP Cyclo Olefin Copolymer (COC)
This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces..
Izod Impact, Unnotched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ASTM D256
Mitsui APELâ„¢ APL6015T Cyclo Olefin Copolymer (COC)
This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces..
Izod Impact, Unnotched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ISO 180/1eU
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY
Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p..
Izod Impact, Unnotched (ISO) 10.0 kJ/m²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
80x10x4mm; ISO 180/1U
SYNTHOS Krasten® 152 General Purpose Polystyrene
Improved heat resistance, very good rheological properties.Examples of Application:Injection moulding – vegetable boxes for refrigerators, shower enclosure panels, CD and DVD cases. Blends with..
Izod Impact, Unnotched (ISO) 10.0 kJ/m²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Lubricomp RL0049 PA 66
LNP* Lubricomp* RL0049 is a compound based on Nylon 66 resin containing PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant.This data was supplied..
Izod Impact, Unnotched (ISO) 10.0 kJ/m²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Stat-kon CX01039 PS (Europe-Africa-Middle East)
LNP* Stat-kon* CX01039 is a compound based on Polystyrene resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP..
Izod Impact, Unnotched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
Shandong Rike Chemical RIKEâ„¢ RK-521 MBS Impact Modifier for PVC Transparent Product
Outline of MBS Impact ModifierRIKEâ„¢ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is ..
Izod Impact, Unnotched (ISO) 10.0 kJ/m²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Stat-kon ZX05009 PPE+PS (Europe-Africa-Middle East)
LNP* Stat-kon* ZX05009 is a compound based on PPE+PS Blend resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the..
Izod Impact, Unnotched (ISO) 10.0 kJ/m²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp CF004 PS (Europe-Africa-Middle East)
LNP* Thermocomp* CF004 is a compound based on Polystyrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Unnotched (ISO) 10.0 kJ/m²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp CF006 PS (Europe-Africa-Middle East)
LNP* Thermocomp* CF006 is a compound based on Polystyrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Unnotched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP WH0270F PBT
LNP* Thermocomp* WH0270F is a dense compound based on PBT.
Izod Impact, Unnotched (ISO) 10.0 kJ/m²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp WH0270FX_WH5A289 PBT
2.7 specific gravity PBTThis data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
Goodfellow TPX® DX845 Extrusion Grade Polymethylpentene
This grade is highly recommended for film extrusion; also for injection molding, fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensiv..
Izod Impact, Unnotched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80x10x4; ISO 180/1U
Eurostar Starglas CF006 Styrenic, 30% Glass Filled, Injection Molding
Starglas CF006 is a 30% Glass Fiber Reinforced Styrenic Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Unnotched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ISO 180/1U
A.D. Compound Adene NCQA Homopolymer 40% CaCO3 Filled Polypropylene
Information provided by A.D. Compound
Izod Impact, Unnotched (ISO) 10.0 - 80.0 kJ/m²
4.76 - 38.1 ft-lb/in²
Average value: 34.7 kJ/m² Grade Count:9
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Izod Impact, Unnotched (ISO) 10.0 - 40.0 kJ/m²
4.76 - 19.0 ft-lb/in²
Average value: 30.8 kJ/m² Grade Count:7
Overview of materials for Acetal Copolymer, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu..
Izod Impact, Unnotched (ISO) 10.0 - 20.0 kJ/m²
4.76 - 9.52 ft-lb/in²
Average value: 16.0 kJ/m² Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo..
Izod Impact, Unnotched (ISO) 10.0 - 90.0 kJ/m²
4.76 - 42.8 ft-lb/in²
Average value: 54.4 kJ/m² Grade Count:29
Overview of materials for Nylon 6, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea..
Izod Impact, Unnotched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP CX94108 PS (Europe-Africa-Middle East)
LNP* LUBRICOMP* CX94108 is a compound based on Polystyrene resin containing Proprietary Lubricant. Added features include: Internally Lubricated.
Copyright © lookpolymers.com All Rights Reserved