| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP THERMOCOMP |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | SABIC Innovative Plastics LNP THERMOCOMP WH0270F PBT.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 2.695 g/cc | 0.09736 lb/in³ | ASTM D792 |
| Moisture Absorption | 0.0800 % | 0.0800 % | 50% RH, 24 hrs; ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.011 cm/cm @Time 86400 sec |
0.011 in/in @Time 24.0 hour |
ASTM D955 |
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm @Time 86400 sec |
0.013 in/in @Time 24.0 hour |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 30.0 MPa | 4350 psi | 5 mm/min; ISO 527 |
| 31.0 MPa | 4500 psi | Type I, 5 mm/min; ASTM D638 | |
| Tensile Strength, Yield | 31.0 MPa | 4500 psi | Type I, 5 mm/min; ASTM D638 |
| 31.0 MPa | 4500 psi | 5 mm/min; ISO 527 | |
| Elongation at Break | 0.70 % | 0.70 % | Type I, 5 mm/min; ASTM D638 |
| 0.70 % | 0.70 % | 5 mm/min; ISO 527 | |
| 0.80 % | 0.80 % | Flexural Strain, break, 2 mm/min; ISO 178 | |
| Elongation at Yield | 0.50 % | 0.50 % | Type I, 5 mm/min; ASTM D638 |
| 0.50 % | 0.50 % | 5 mm/min; ISO 527 | |
| Tensile Modulus | 8.28 GPa | 1200 ksi | 1 mm/min; ISO 527 |
| 10.46 GPa | 1517 ksi | 5 mm/min; ASTM D638 | |
| Flexural Yield Strength | 52.0 MPa | 7540 psi | 2 mm/min; ISO 178 |
| 56.0 MPa | 8120 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Flexural Modulus | 8.32 GPa | 1210 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 8.32 GPa | 1210 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 0.190 J/cm | 0.356 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 3.00 kJ/m² | 1.43 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 10.0 kJ/m² | 4.76 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 43.3 - 45.3 µm/m-°C @Temperature -30.0 - 30.0 °C |
24.1 - 25.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E 831 |
| CTE, linear, Transverse to Flow | 57.5 - 59.5 µm/m-°C @Temperature -30.0 - 30.0 °C |
31.9 - 33.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM E 831 |
| Deflection Temperature at 1.8 MPa (264 psi) | 162 °C | 324 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 164 °C @Thickness 3.20 mm |
327 °F @Thickness 0.126 in |
unannealed; ASTM D648 |