| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® HF500R PC (Europe-Africa-Middle East)
LEXAN HF500R is an easy flow, 9% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance and impact performance.
|
|||
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | ISO 180 |
|
Iran Petrochemical (PCC) EP-C 30 R Polypropylene
The grade is a heterophasic polypropylene copolymer for injection molding the product offers an excellent balance of stiffness.Application: automotive parts, wells, garden furniture, chair shells an..
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature -30.0 °C
|
3.81
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL SE1GFN2 PPE+PS (Asia Pacific)
PPE+PS blend. 20% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. Dielectric strength. Dimensional stability. Suitable for E/E applications.
|
|||
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | ISO 180/1eA |
|
Solvay TECHNYL® A 238 V13 PA66, 13% glass fiber, DRY
Description: Polyamide 66, reinforced with 13% of glass fiber, heat stabilized, with improved impact resistance, for injection molding.Available in: Europe, Latin America and North AmericaProduct Ap..
|
|||
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL159 PA 66
LNP* LUBRICOMP* RFL159 is a compound based on Nylon 66 resin containing 25% Glass Fiber, 5% PTFE. Added features of this material include: Wear Resistant, Flame Retardant
|
|||
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP LUBRICOMP ZFG26 PPE+PS
LNP* LUBRICOMP* ZFG26 is a compound based on PPE+PS resin containing 30% Glass Fiber, 10% Graphite. Added features of this material include: Wear Resistant.
|
|||
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON DE0026 PC (Europe-Africa-Middle East)
LNP* Stat-kon* DC-1002 FR is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Flame Retardant, Electrically Conductive.
|
|||
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON DE003Z PC
LNP STAT-KON* DE003Z is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Extrusion Grade.
|
|||
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON DEL13PXC PC (Europe-Africa-Middle East)
LNP* Stat-kon* DEL13PXC is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Superior Molding.
|
|||
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | Notch A; ISO 180 |
|
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® BR111 is a natural-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outstanding chemical..
|
|||
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® 4022 PBT (Europe-Africa-Middle East)
VALOX 4022 is a 20% high strength glass fibre reinforced PBT injection moulding resin, with improved mechanical properties. Applications : Spotlights, appliance housings and handles.
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature 0.000 °C
|
3.81
ft-lb/in² <br>@Temperature 32.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® ENH4550 PBT (Europe-Africa-Middle East)
25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin.
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature 23.0 °C
|
3.81
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Xylex X8300HP PC+POLYESTER (Europe-Africa-Middle East)
Transparent, US Food Contact compliant, chemically resistant.
This grade will no longer be supported with biocompatibility information and should not be used for medical applications which require b..
|
|||
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP DF002 PC
LNP THERMOCOMP* DF002 is a compound based on Polycarbonate resin containing 10% Glass Fiber.
|
|||
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP PDXE98480 PEI
LNP* Thermocomp* PDXE98480 is a compound based on Polyetherimide with Proprietary Fillers. Added feature of this grade: Reinforced.
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature -30.0 °C
|
3.81
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA (Asia Pacific)
Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-..
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature -30.0 °C
|
3.81
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
|
|||
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON DX06500 PC
LNP* STAT-KON* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive, Wear Resistant, Easy ..
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature -30.0 °C
|
3.81
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature -30.0 °C
|
3.81
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® V3900WX PBT+PC
PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance.
|
|||
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP MF002S PP (Europe-Africa-Middle East)
LNP* THERMOCOMP* MF002S is a compound based on Polypropylene resin containing Glass Fiber. Added features include: Heat Stabilized.
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature -40.0 °C
|
3.81
ft-lb/in² <br>@Temperature -40.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL LTA6020 PPE+PS (Europe-Africa-Middle East) |
|||
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | ISO 180-93 |
|
Wellman Wellamid® GF33-66 XE-BKDX9 33% Glass Fiber Reinforced Nylon 66
Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman.
|
|||
| Izod Impact, Notched (ISO) |
8.00
kJ/m² <br>@Temperature -30.0 °C
|
3.81
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1A |
|
DuPont Performance Polymers Crastin® SK603 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Crastin SK603 NC010 is a 20% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P..
|
|||
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80x10x4; ISO 180/1A |
|
Eurostar Staramide RFB24 PA66, 20/10% Glass Fiber/Glass Bead Filled Injection Molded
RFB24 is a Glass Bead and Glass Fiber Reinforced, Polyamide 66 Injection Molding Resin (also known as Staramide 66 2010VK Z3)Information provided by Polymer Technology & Services, the North American..
|
|||
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | ISO 180/1A |
|
Chi Mei Polyrex® PH-888H Polystyrene - High Impact
High FDI; high heat
|
|||
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | ASTM D256 |
|
BLUESTAR 201-G20202 PBT, 20% Glass Filled
Typical Applications: Energy saving lighting, E/E applicationsInformation provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-KON REF42 PA 66 (Asia Pacific)
LNP* Stat-kon* REF42 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Fiber.
|
|||
| Izod Impact, Notched (ISO) |
8.00
-
10.0
kJ/m² <br>@Temperature -30.0 - -30.0 °C
|
3.81
-
4.76
ft-lb/in² <br>@Temperature -22.0 - -22.0 °F
|
Average value: 9.33 kJ/m² Grade Count:2 |
|
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..
|
|||