| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled |
| Manufacturer | BASF |
| Trade Name | Ultradur B |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | BASF Ultradur B 4300 G6 LS BK15073 30% Glass Filled PBT.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
| Water Absorption | 0.20 % | 0.20 % | 24 hour; ISO Test |
| 0.40 % | 0.40 % | ISO 62 | |
| Moisture Absorption at Equilibrium | 0.20 % | 0.20 % | 23°C/50% R.H.; ISO 62 |
| Viscosity Test | 101 cm³/g | 101 cm³/g | Viscosity number |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 135 MPa | 19600 psi | 5mm/min; ISO 527 |
| Elongation at Break | 2.7 % | 2.7 % | 5mm/min; ISO 527 |
| Flexural Modulus | 8.60 GPa | 1250 ksi | ISO Data |
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | ISO Test |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 223 °C | 433 °F | 10 K/min |
| 223 °C | 433 °F | ASTM Test | |
| Deflection Temperature at 1.8 MPa (264 psi) | 206 °C | 403 °F | ISO 75 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | BK15073 | |
| Commercial Status | North America and Europe | |
| Impact Modified | No | |
| Primary Processing Technique | Injection Molding | |
| Special characteristic | Heat stabilized or stable to heat |