Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 49.0 MPa | 7110 psi | ISO METHOD 176 |
NYCOA 2012 Copolymer Nylon easy flowing, exceptional toughness and flexibility with lower water absorptionInformation provided by NYCOA, Inc. |
|||
Flexural Yield Strength | 49.0 - 69.0 MPa | 7110 - 10000 psi | Average value: 65.8 MPa Grade Count:13 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Flexural Yield Strength | 49.0 - 151 MPa | 7110 - 21900 psi | Average value: 74.3 MPa Grade Count:21 |
Overview of materials for ABS/Polyester Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Flexural Yield Strength | 49.0 MPa @Thickness 3.20 mm |
7110 psi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical LI931 Extrusion ASA Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical |
|||
Flexural Yield Strength | 49.0 MPa | 7110 psi | DIN 53455; ASTM D790 |
Kolon KOPA® KN170SA General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Yield Strength | 49.0 MPa | 7110 psi | DIN 53455; ASTM D790 |
Kolon KOPEL® KP3340 General Purpose TPE Resin KOPEL® is a thermoplastic polyester elastomer which is a new engineering rubber having combined properties of conventional rubber and thermoplastic. Its flexibility and elastic recovery are very.. |
|||
Flexural Yield Strength | 49.0 MPa | 7100 psi | ASTM D790 |
Spartech Royalstatâ„¢ R63 ABS/PVC Static Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 49.0 MPa | 7110 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 4X08423 FP-P (PFA) LNP* THERMOCOMP* 4X08423 is a compound based on PFA resin containing Glass Fiber. |
|||
Flexural Yield Strength | 49.0 MPa | 7110 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP C1000XXP PS (Europe-Africa-Middle East) LNP* THERMOCOMP* C1000XXP is a compound based on Polystyrene resin. Added features include: High Impact. |
|||
Flexural Yield Strength | 49.0 MPa | 7110 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOTUF RN001IX4 PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RN001X4 is a compound based on PA 66 resin containing MoS2. Added features include: Internally Lubricated, High Impact, Heat Stabilized. |
|||
Flexural Yield Strength | 49.0 MPa | 7110 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP PPE+PP blend. Suitable for painted exterior automotive applications. |
|||
Flexural Yield Strength | 49.0 MPa | 7110 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP (Asia Pacific) PPE+PP blend. Suitable for painted exterior automotive applications. |
|||
Flexural Yield Strength | 49.0 MPa | 7110 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP AW00A ABS (Europe-Africa-Middle East) LNP* THERMOCOMP* AW00A is a compound based on Acrylonitrile Butadiene Styrene resin containing Wollastonite. |
|||
Flexural Yield Strength | 49.0 MPa | 7110 psi | ASTM D790 |
Samyang Trimma® SD6320 PMMA, Translucent High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Applications: Laptop, Monitor Front Cover - for high flow, high gloss and high hardnessInformat.. |
|||
Flexural Yield Strength | 49.0 MPa | 7110 psi | ASTM D790 |
Tipco Tipcolene® FPT 30 - 30% Talc Reinforced Polypropylene Homopolymer Compound 30% Talc Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Yield Strength | 49.0 MPa | 7110 psi | ASTM D790 |
Cheng Yu Plastic PP225 Flame Retardant Polypropylene, Medium Impact |
|||
Flexural Yield Strength | 49.0 MPa | 7110 psi | ASTM D790 |
Cheng Yu Plastic PP228H TALC 10 Polypropylene, 10% Talc, High Heat |
|||
Flexural Yield Strength | 49.0 MPa | 7100 psi | ASTM D790 |
Clariant Renol CAB1000 Cellulose Acetate Butyrate Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 49.0 MPa | 7110 psi | ASTM D790 |
Cheng Yu Plastic BK1021 Electric Conducting Polypropylene, Extrusion |
|||
Flexural Yield Strength | 49.0 MPa | 7110 psi | ASTM D790 |
Ineos Nova 5540 High Impact Polystyrene
(discontinued **) Excellent balance of toughness, flow, and set-up, High gloss, USP Class VIApplications: Structural foam, Housewares, Toys, Appliance parts, Dairy containersProperties were determined on injection mo.. |
|||
Flexural Yield Strength | 49.0 MPa | 7110 psi | ASTM D790 |
Ineos Nova 6100 Super High Impact Polystyrene
(discontinued **) Good balance of gloss and impact, High glossApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection molded specimen.. |
|||
Flexural Yield Strength | 49.0 MPa | 7110 psi | ASTM D790 |
Ineos Nova 6110 Super High Impact Polystyrene
(discontinued **) Good balance of gloss and impact, High glossApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection molded specimen.. |
|||
Flexural Yield Strength | 49.0 MPa | 7110 psi | ASTM D790 |
Eastman Tenite Butyrate 465E2R30008 Natural, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Flexural Yield Strength | 49.0 MPa | 7110 psi | ASTM D790 |
Eastman Tenite Butyrate 465E3720008 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Flexural Yield Strength | 49.0 MPa | 7110 psi | ASTM D790 |
Eastman Tenite Butyrate 513E3720012 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Flexural Yield Strength | 49.0 MPa | 7100 psi | ASTM D790 |
PlastxWorld DAICEL STYROL® GW30 HIPS UV stable flame retarded HIPSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 49.0 MPa | 7110 psi | ASTM D790 |
PlastxWorld DAICEL STYROL® SK60 HIPS UV stable flame retarded HIPSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |