Material Notes:
easy flowing, exceptional toughness and flexibility with lower water absorptionInformation provided by NYCOA, Inc.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183-A
Water Absorption 1.0 %
1.0 %
ISO METHOD 62
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.0 MPa
8410 psi
ISO METHOD 527
Elongation at Break >= 300 %
>= 300 %
ISO METHOD 527
Flexural Yield Strength 49.0 MPa
7110 psi
ISO METHOD 176
Flexural Modulus 1.172 GPa
170.0 ksi
ISO METHOD 178
Izod Impact, Notched 1.13 J/cm
2.12 ft-lb/in
ISO METHOD 180
Thermal Properties Metric English Comments
Melting Point 205 °C
401 °F
ISO METHOD 3146C
Processing Properties Metric English Comments
Processing Temperature 250 °C
482 °F
Rear Barrel Temperature 210 °C
410 °F
Middle Barrel Temperature 230 °C
446 °F
Front Barrel Temperature 250 °C
482 °F
Nozzle Temperature 250 °C
482 °F
Mold Temperature 80.0 °C
176 °F
Drying Temperature 76.0 °C
169 °F