| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Shear Strength |
65.0
MPa <br>@Temperature 22.0 °C
|
9430
psi <br>@Temperature 71.6 °F
|
0° |
|
Hexcel® HexPly® 954-3 Curing Cyanate Resin, YSH-60A Fiber
Information provided by HexCel
|
|||
| Shear Strength | 65.0 MPa | 9430 psi | 0°, Short Beam |
|
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass UD fabric 315 g/m2
Information provided by HexCel
|
|||
| Shear Strength | 65.0 MPa | 9430 psi | 0º, ILSS Short Beam, RT, Dry; EN2563 |
|
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 50%/G939 HS Carbon
Information provided by HexCel
|
|||
| Shear Strength | 65.0 MPa | 9430 psi | ILSS; EN2563 |
|
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/40%/285T2/AS4C-6K
Fiber: AS4C, Weave: 2x2T, 295 g/m2Information provided by HexCel
|
|||
| Shear Strength | 65.0 MPa | 9430 psi | ASTM D732 |
|
Ashley Polymers Ashlene® 528L Nylon 66
General purpose injection molding grade.Data provided by the manufacturer
|
|||
| Shear Strength | 65.0 MPa | 9430 psi | ASTM D732 |
|
Ashley Polymers Ashlene® 528LW Nylon 66
General purpose injection molding grade.Data provided by the manufacturer
|
|||