Material Notes:
Fiber: AS4C, Weave: 2x2T, 295 g/m2Information provided by HexCel
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
Cured Resin
1.48 g/cc
0.0535 lb/in³
Nominal Laminate
1.79 g/cc
0.0647 lb/in³
Fibre
Mechanical Properties Metric English Comments
Tensile Strength, Yield 787 MPa
114000 psi
EN2597B
Tensile Modulus 67.0 GPa
9720 ksi
EN2597B
Compressive Yield Strength 807 MPa
117000 psi
EN2850B
Compressive Modulus 58.0 GPa
8410 ksi
EN2850B
Shear Modulus 3.70 GPa
537 ksi
EN6031
Shear Strength 65.0 MPa
9430 psi
ILSS; EN2563
99.0 MPa
14400 psi
In-Plane; EN6031
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 194 °C
381 °F
EN6032
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.0314
Fiber Volume (%) 49.5