Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 11.72 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 11.72 GPa
1700 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DFL28 PC
LNP* Lubricomp* DFL28 is a compound based on Polycarbonate resin containing 40% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated.
Flexural Modulus 11.72 GPa
1700 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DFL28 PC (Asia Pacific)
LNP* Lubricomp* DFL28 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 11.72 GPa
1700 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 2400 PEI
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. WRAS certification in recognized colors.
Flexural Modulus 11.72 GPa
1700 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 2400 PEI (Asia Pacific)
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. WRAS certification in recognized colors.
Flexural Modulus 11.72 GPa
1700 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 2410 PEI
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
Flexural Modulus 11.72 GPa
1700 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 2410 PEI (Asia Pacific)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
Flexural Modulus 11.72 GPa
1700 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 2410R PEI
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
Flexural Modulus 11.72 GPa
1700 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 2410R PEI (Asia Pacific)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
Flexural Modulus 11.72 GPa
1700 ksi
2.6 mm/min, 100 mm span; ASTM D 790
SABIC Innovative Plastics Ultem 3451 PEI
45% Glass fiber and mineral filled, standard flow Polyetherimide (Tg 217C) with enhanced dimensional stability. ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 11.72 GPa
1700 ksi
2.6 mm/min, 100 mm span; ASTM D 790
SABIC Innovative Plastics Ultem 3451 PEI (Asia Pacific)
45% Glass fiber and mineral filled, standard flow Polyetherimide (Tg 217C) with enhanced dimensional stability. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 11.72 GPa
1700 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM HU2400 PEI
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food..
Flexural Modulus 11.72 GPa
1700 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM HU2400 PEI (Asia Pacific)
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food..
Flexural Modulus 11.72 GPa
1700 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DX06500 PC (Asia Pacific)
LNP* Stat-kon* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
Flexural Modulus 11.72 GPa
1700 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON EE003XXC PEI
LNP STAT-KON* EE003XXC is a compound based on Polyetherimide resin containing 15% Carbon Fiber. Added features of this material include: Clean Compound System, Electrically Conductive.
Flexural Modulus 11.72 GPa
1700 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON EE003XXC PEI (Asia Pacific)
LNP* STAT-KON* EE003XXC is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Clean Compounding System.
Flexural Modulus 11.72 GPa
1700 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp EF008E PEI
LNP* Thermocomp* EF008E is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas..
Flexural Modulus 11.72 GPa
1700 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp EF008E PEI (Asia Pacific)
LNP* Thermocomp* EF008E is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pac..
Flexural Modulus 11.72 GPa
1700 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DX06500 PC
LNP* STAT-KON* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive, Wear Resistant, Easy ..
Flexural Modulus 11.72 GPa
1700 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Ultem HU2400 PEI (Europe-Africa-Middle East)
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food..
Flexural Modulus 11.72 GPa
1700 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP AH0400A ABS
LNP* THERMOCOMP* AH0400A is a compound based on ABS resin. Added feature of this material is: High Specific Gravity.
Flexural Modulus 11.72 GPa
1700 ksi
ASTM D790
SABIC Innovative Plastics LNP VERTON RV008ES PA 66
LNP* VERTON* RV008ES is a compound based on Nylon 66 resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
Flexural Modulus 11.72 GPa
1700 ksi
ASTM D790
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 (Asia Pacific)
LNP* Verton* RV008ES is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Flexural Modulus 11.72 GPa
1700 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RF0069XZ PA 66 (Asia Pacific)
LNP* THERMOCOMP* RF0069XZ is a compound based on Nylon 66 resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.
Copyright © lookpolymers.com All Rights Reserved