Mechanical Properties Metric English Comments
Flexural Modulus 11.7 GPa
1700 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 FR compound
Flexural Modulus 11.7 GPa
1700 ksi
Crosswise; ASTM D790
G-9 Fiberglass Melamine Laminate Sheet
This material is very hard, flame resistant, and has excellent electrical properties. G-9 has high arc and heat resistance and is recommended for humid environments. It is used for switch board pane..
Flexural Modulus 11.7 - 13.8 GPa
1700 - 2000 ksi
ASTM D790
Mar-Bal MB2000-20 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
Flexural Modulus 11.72 GPa
1700 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 2410 PEI
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
Flexural Modulus 11.72 GPa
1700 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 2410 PEI (Asia Pacific)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
Flexural Modulus 11.72 GPa
1700 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics ULTEM 2410R PEI
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
Flexural Modulus 11.7 GPa
1700 ksi
ASTM D790
Solvay Specialty Polymers Amodel® A-1133 NL WH 505 Polyphthalamide (PPA), 33% Glass Fiber
Amodel® A-1133 NL resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib..
Flexural Modulus 11.72 GPa
1700 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM HU2400 PEI
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food..
Flexural Modulus 11.7 GPa
1700 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON DX13320C PC COPOLYMER (Asia Pacific)
LNP* Statkon DX13320C is ultra clean polycarbonate/carbon fiber compound with high modulus, good flow ability, easy mold release, and high level of cleanliness for the most demanding application. A ..
Flexural Modulus 11.72 GPa
1700 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp EF008E PEI
LNP* Thermocomp* EF008E is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas..
Flexural Modulus 11.7 GPa
1700 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP WH0450E PBT
LNP* Thermocomp* WH0450E is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Flexural Modulus 11.7 GPa
1700 ksi
ASTM D790
Sumitomo Bakelite North America 73-70-70 C-P /73-70-70 VO-P Short-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I..
Flexural Modulus 11.7 GPa
1700 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Asia Pacific)
Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
Flexural Modulus 11.72 GPa
1700 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DX06500 PC
LNP* STAT-KON* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive, Wear Resistant, Easy ..
Flexural Modulus 11.72 GPa
1700 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Ultem HU2400 PEI (Europe-Africa-Middle East)
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food..
Flexural Modulus 11.72 GPa
1700 ksi
ASTM D790
SABIC Innovative Plastics LNP VERTON RV008ES PA 66
LNP* VERTON* RV008ES is a compound based on Nylon 66 resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
Flexural Modulus 11.72 GPa
1700 ksi
ASTM D790
SABIC Innovative Plastics LNP VERTON RV008ES PA 66 (Asia Pacific)
LNP* Verton* RV008ES is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Bulk Molding Compounds BMC 1403 Electrical Grade
BMC 1403 is one of the most useful general-purpose electrical grade materials available on the market. Competitive against phenolic, melamine, and urea materials for electrical applications. Easy mo..
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Bulk Molding Compounds BMC 1603 Multi-purpose grade
BMC 1603 is a multi-purpose, moderate strength, low cost material that is suitable for injection, compression and transfer molding. UL® recognized. This material was formerly known as Glastic® 160..
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Bulk Molding Compounds BMC A50-XHS High Strength Grade Molding Compound
BMC A50-XHS is a high strength bulk molding compound. Due to the excellent flow and controlled reactivity, BMC A50-XHS is well suited for injection, transfer or compression molding. Typical applic..
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Bulk Molding Compounds BMC 400 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade
BMC 400 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, and power tool housings.
Flexural Modulus 11.7 GPa
1700 ksi
ASTM D790
Techmer ES Statiblend® PPS GF23 IM BK 23% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 23% Filler by WeightAdditive: Impact ModifierFeatures: Conductive and Impact ModifiedAppearance: BlackInformation provided..
Flexural Modulus 11.72 GPa
1700 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RF0069XZ PA 66 (Asia Pacific)
LNP* THERMOCOMP* RF0069XZ is a compound based on Nylon 66 resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.
Flexural Modulus 11.7 GPa
1700 ksi
Tangent, 0.125 in; ASTM D790
Matrixx Group 80M7451 45% Glass/Mineral Filled PET  (discontinued **)
Data provided by The Matrixx Group, formerly RePlas.
Flexural Modulus 11.7 GPa
1700 ksi
ISO 178
SABIC Innovative Plastics LNP VERTON NV008E PC/ABS (Asia Pacific)
LNP* Verton* NV008E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding.