Polymer Property : Flexural Modulus = 8.09 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 8.09 GPa
1170 ksi
ASTM D 790
SABIC Innovative Plastics Valox® 553M PBT+PC (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 8.09 GPa
1170 ksi
ASTM D 790
SABIC Innovative Plastics Valox® PDR4908 PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 8.09 GPa
1170 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK
LNP* THERMOCOMP* LF004E is a compound based on Polyetheretherketone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding.