Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 115 - 120 °C | 239 - 248 °F | |
Oceanchem Group 3,5-dibromo-4-(2,3-dibromopropoxy) diphenyl sulfone (Octabromobisphenol S) Molecular Formula: C18H14O4SBr8Cas No.: 42757-55-1Use: Mainly used for plastic as flame-retardant, widely for PP, PE, PS, ABS resin rubber and the stability is very best.Information Provided by Ocea.. |
|||
Melting Point | 117 - 120 °C | 243 - 248 °F | |
Pau Tai Super fine zinc stearate, Monomer Stabilizer Non-toxic stabilizer, grain diameter:600 mesh,90% has passed.Applications: Applicable to printing ink, rubber and coating products. |
|||
Melting Point | 117 - 120 °C | 243 - 248 °F | |
Pau Tai Zinc stearate, Monomer Stabilizer Non sulfide staining and non-toxic. Excellent internal lubricity and good gelation property.Applications: Lubricant of non-toxic, plastic and rubber products. |
|||
Melting Point | 100 - 120 °C | 212 - 248 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 115 Linear Thermoplastic Polyurethane
(discontinued **) PEARLBOND® 115 is a linear, aromatic polyurethane, supplied in form of white slightly yellowish pellets, which combines a very high crystallization rate with a high thermoplasticity level.Applicati.. |
|||
Melting Point | 90.0 - 120 °C | 194 - 248 °F | TMA Melt Range |
Huntsman IROGRAN® CA116-201 TPU-Polyester Introduction: IROGRAN CA116-201 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-201 is part of the HUNTSMAN film and shee.. |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | |
Fine Organics FINAWAX VL Lubricant Additive Applications: Antiblock agent for soft PVC calendered films/sheets, specially for printed films with antiblocking properties.Information provided by Fine Organics |
|||
Melting Point | 117 - 120 °C | 243 - 248 °F | |
Indium Corp. Indalloy 62 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 105 - 120 °C | 221 - 248 °F | DSC |
EMS-Griltech Griltex® D 1260 A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 115 - 120 °C | 239 - 248 °F | DSC |
EMS-Griltech Griltex® D 1619E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | DSC |
EMS-Griltech Griltex® D 1694A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | DSC |
EMS-Griltech Griltex® D 1712A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | Sheath |
EMS-Griltech Grilon® BA 115 White Nylon 6/CoPA Bi-Component Fiber Description: GRILON BA 115 is the new core / sheath bi-component fiber based on PA 6/CoPA with a sheath melting range from 110 - 120 °C. The fine count bi-component fiber guarantees an even distrib.. |
|||
Melting Point | 115 - 120 °C | 239 - 248 °F | Optical birefringence |
Arkema Group PLATAMID® H106 PA80 Powder Copolyamide Platamid® H106 PA powder is a special purpose, medium melting point, very low viscosity, thermoplastic copolyamide adhesive suitable for thermal bonding and laminating of textile and foam substrate.. |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | DSC |
BASF Ecoflex® 1200 F Blend Biodegradable Polyester Description: A flexible plastic designed for film extrusion and extrusion coating. Ecoflex® F Blend 1200 comes closer than any other biodegradable plastic to the processing properties of LDPE and L.. |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | 10 K/min |
BASF Ecoflex® F BX 7011 Biodegradable Plastic A flexible plastic designed for film extrusion and extrusion coating. Ecoflex F BX 7011 comes closer than any other biodegradable plastic to the processing properties of LDPE and LLDPE. Blown film e.. |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | DSC |
BASF Ecovio® C2224 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2224 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | DSC |
BASF Ecoflex® C1200 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2332 is our biodegradable, statistical, aliphatic-aromatic copolyester based on the monomers 1,4-butanediol, adipic acid and terephathalic acid in the polymer chain. E.. |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | DSC |
BASF Ecoflex® P BX 7020 Biodegradable Polyester Description: Ecoflex® P BX 7020 is our biodegradable, statistical, aliphatic-aromatic copolyester based on the monomers 1,4-butanediol, adipic acid and terephthalic acid or dimethyltherephthalate i.. |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | DSC |
BASF Ecovio® C2203 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2203 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |