Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Ecoflex® C1200 F Blend Biodegradable Polyester

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyester, TP
Manufacturer BASF
Trade Name Ecoflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ecoflex® C1200 F Blend Biodegradable Polyester.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Ecovio® F Blend C2332 is our biodegradable, statistical, aliphatic-aromatic copolyester based on the monomers 1,4-butanediol, adipic acid and terephathalic acid in the polymer chain. Ecoflex® F Blend C1200 will biodegrade to the basic monomers 1,4-butanediol, adipic acid and terephthalic acid and eventually to carbon dioxide, water and biomass when metabolized in the soil or compost under standard conditions.Applications: Ecoflex® F Blend C1200 has been developed for the conversion to flexible films using a blown film or cast film process. Typical applications are packaging films, agricultural films and compost bags, In view of numerous factors influencing functionality and shelf life of Ecoflex® films and finished articles made thereof these parameters have to be tested by the converters before utilization.Information provided by BASF
Physical Properties Metric English Comments
Density 1.25 - 1.27 g/cc
0.0452 - 0.0459 lb/in³
ISO 1183
Water Vapor Transmission 140 g/m²/day
9.02 g/100 in²/day
DIN 53122
Oxygen Transmission Rate 1600 cc/m²/day
103 cc/100 in²/day
DIN 53380
Melt Flow 2.7 - 4.9 g/10 min
2.7 - 4.9 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 32
32
ISO 868
Tensile Strength 35.0 - 44.0 MPa
5080 - 6380 psi
ISO 527
Tensile Strength, Ultimate 36.0 - 45.0 MPa
5220 - 6530 psi
ISO 527
Elongation at Break 560 - 710 %
560 - 710 %
ISO 527
Thermal Properties Metric English Comments
Melting Point 110 - 120 °C
230 - 248 °F
DSC
Vicat Softening Point 91.0 °C
196 °F
A/50; ISO 306
Optical Properties Metric English Comments
Transmission, Visible 82 %
82 %
ASTM D1003
Descriptive Properties Value Comments
Commercial Status Europe
Users viewing this material also viewed the following: