| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 220 °C | 428 °F | DSC |
|
PolyOne Nymax™ ND633 GF Black Polyamide 6 (Nylon 6)
The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en..
|
|||
| Melting Point | 220 °C | 428 °F | DSC; STN EN ISO 3146 |
|
Plastcom SLOVAMID 6 G 10 Polyamide 6, 10% Graphite
FeaturesPA 6 for injection moulding with addition of 10% graphite, the PA surface rolling resistance force is significantly lowered. Used mainly in the product of crates and cases for bearings, sli..
|
|||
| Melting Point | 220 °C | 428 °F | |
|
Plastcom SLOVAMID 6 GF 10 GB 20 PA6, 10% glass fibre, 20% glass beads
FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fibre and 20% glass beads. Application: impacted mouldings and mouldings with high strength applied in automotive, electri..
|
|||
| Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1/-3 |
|
DSM Akulon® Ultraflow™ K-FKGS6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry)
(discontinued **
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Melting Point | 220 °C | 428 °F | ASTM D3418 |
|
Honeywell Aegis™ H135XP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **)
Description: Aegis H135XP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon..
|
|||
| Melting Point | 220 °C | 428 °F | 10 K/min |
|
BASF Capron® B135ZP Nylon 6 (DAM)
(discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
|
|||
| Melting Point | 220 °C | 428 °F | DIN 53736; ASTM D789 |
|
Kolon KOPA® KN136 General Purpose Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
|
|||
| Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1,-3 |
|
Gromax BFG30-B103N1 Nylon 6 33% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1,-3 |
|
Gromax BFG45-DN00N1 Nylon 6 46% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1,-3 |
|
Gromax BFM30-EL04B2 Nylon 6 30% Mineral Filled (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1,-3 |
|
Gromax BTQ80-AQ00N1 Nylon 6, Impact Modified (Conditioned)
Information provided by Gromax Enterprises Corp.
|
|||
| Melting Point | 220 °C | 428 °F | ISO 3146 |
|
Wellman Wellamid® MRGF25/15 42H-GY1 40% Mineral/Glass Fiber Reinforced Nylon 6
Description: Mineral/Glass Fiber Reinforced Nylon 6Information provided by Wellman.
|
|||
| Melting Point | 220 °C | 428 °F | 10°C/min (DAM); ISO 11357-1/-3 |
|
DSM Akulon® K222-KMV5 Nylon 6-25% Mineral Reinforced (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Melting Point | 220 °C | 428 °F | 10°C/min (DAM); ISO 11357-1/-3 |
|
DSM Akulon® K222-KWGV4 Nylon 6-20% Glass Reinforced (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1/-3 |
|
DSM Akulon® K224-G3 (Dry) 15% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Melting Point | 220 °C | 428 °F | 10°C/min (DAM); ISO 11357-1/-3 |
|
DSM Akulon® Ultraflow™ K-FHG6 Nylon 6-30% Glass Reinforced (European Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Melting Point | 220 °C | 428 °F | ISO 3146 |
|
Azoty Tarnow™ Alphalon™ 36 Nylon 6
A bright polyamide 6 grade of medium viscosity that is suited for the production of films and monofilaments.Information provided by ATT Polymers™
|
|||
| Melting Point | 220 °C | 428 °F | 10 K/min |
|
BASF Ultramid® 8202 HS BK-102 PA6 (Dry)
Ultramid 8202 HS BK-102 is an unfilled, heat stabilized, pigmented black, low viscosity, general purpose injection molding PA6 exhibiting excellent fluidity for filling thin sections. It possesses ..
|
|||
| Melting Point | 220 °C | 428 °F | 10 K/min |
|
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Dry)
Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The gla..
|
|||
| Melting Point | 220 °C | 428 °F | ASTM Test |
|
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Conditioned)
Ultramid 8234G HS is a heat stabilized, 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensio..
|
|||
| Melting Point | 220 °C | 428 °F | ASTM Test |
|
BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Conditioned)
Ultramid 8272G HS BK-102 is a 12% glass fiber reinforced, black pigmented, thermally modified, nylon 6 blow molding compound offering an excellent balance of engineering properties combined with the..
|
|||
| Melting Point | 220 °C | 428 °F | 10 K/min |
|
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Conditioned)
Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a
balance of st..
|
|||
| Melting Point | 220 - 225 °C | 428 - 437 °F | DSC; ISO 11357-3 |
|
BASF Ultradur® B 6550 LN PBT
Description: High-viscosity grades for the extrusion of loose buffer tubes for optical fibers, semi-finished products for machining, profiles and pipes.Information provided by BASF
|
|||
| Melting Point | 220 °C | 428 °F | ASTM and ISO test |
|
BASF Capron® 8333G HI HS BK-102 Impact Modified, 33% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron 8333G HI HS BK-102 is a 33% glass reinforced, impact modified polyamide 6 injection molding compound pigmented black developed for applications requiring improved dry as molded toughness in c..
|
|||
| Melting Point | 220 °C | 428 °F | ASTM and ISO test |
|
BASF Capron® BU50I Ultratough Nylon 6 (Dry)
(discontinued **)
Capron Ultratough Nylon BU50I is an unfilled nylon 6 product that maintains its impact strength and ductility to -40 deg F (-40 deg C). The extreme low temperature tolerance of Ultratough Nylon BU5..
|
|||
| Melting Point | 220 °C | 428 °F | |
|
Plastcom SLOVAMID 6 FRC 2 TS PA6, flame retardant, heat stability
FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre..
|
|||
| Melting Point | 220 °C | 428 °F | |
|
Plastcom SLOVAMID 6 NG GF 20 PA6, 20% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 20% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and..
|
|||
| Melting Point | 220 °C | 428 °F | ISO 3146 |
|
BASF Nypel® 2314 HS BK6 PA6 (Dry)
Description: Nypel® 2314 HS BK6 is a black pigmented, low viscosity, heat stabilized, semi crystalline, injection molding compound based on recycled PA6 feedstocks. It also offers the following: go..
|
|||
| Melting Point | 220 °C | 428 °F | |
|
Plastcom SLOVAMID 6 NG GF 30 LS PA6, 30% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 30% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and..
|
|||
| Melting Point | 220 °C | 428 °F | DIN 53765 |
|
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Dry)
Ultramid B3WG6 is a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade.
|
|||