| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 220 °C | 428 °F | |
|
Plastcom SLOVAMID 6 FRM 1 PA6, flame retardant
FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre..
|
|||
| Melting Point | 220 °C | 428 °F | DSC; STN EN ISO 3146 |
|
Plastcom SLOVAMID 6 GF 40 Polyamide 6, 40% Glass Fiber
FeaturesPA 6 for injection moulding, chemically strengthened with 40% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
|
|||
| Melting Point | 220 °C | 428 °F | |
|
Omnia Plastica Omniamid PA6 GHR - HR - at 50% RH
Cast nylon 6 produced with the addition of graphite and a special lubricator which gives to this product better properties than natural PA6G. Whilst retaining the general features of OMNIAMID G it i..
|
|||
| Melting Point | 220 °C | 428 °F | ISO 11357-1 |
|
Radici Radilon® S 35FL (dry) Nylon 6
Radilon® S (homopolyamides) are normally used in cast and blown extrusion for the production of packaging films. Radilon® S grades can be extruded to a thickness varying from 20 mm to 100 mm.Appl..
|
|||
| Melting Point | 220 °C | 428 °F | (Dry) |
|
BASF Capron® GR15 HS 15% Glass-Filled Nylon 6 (Conditioned)
(discontinued **)
Capron GR15 HS is a heat stabilized 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest..
|
|||
| Melting Point | 220 °C | 428 °F | 10°C/min (DAM); ISO 11357-1/-3 |
|
DSM Akulon® K-FHGM24 (Cond.) 30% Glass/Mineral Reinforced, Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1/-3 |
|
DSM Akulon® K224-HG8 Nylon 6-40% Glass Reinforced (European Grade) (Dry)
(discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Melting Point | 220 °C | 428 °F | 10°C/min (DAM); ISO 11357-1/-3 |
|
DSM Akulon® Ultraflow™ K-FG12 Nylon 6-60% Glass Reinforced (European Grade) (Cond)
(discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Melting Point | 220 °C | 428 °F | ASTM D3418 |
|
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR..
|
|||
| Melting Point | 220 °C | 428 °F | DIN 53736; ASTM D789 |
|
Kolon KOPA® KN111 General Purpose Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
|
|||
| Melting Point | 220 °C | 428 °F | ASTM D3418 |
|
LG Chemical LUMID GP2151AF PA6+GF15%, Flame Retardant
Feature: Injection Molding, PA6+GF15%, Flame RetardantApplication: ConnectorsCAS No. 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical
|
|||
| Melting Point | 220 °C | 428 °F | ASTM D3418 |
|
LG Chemical LUMID HI1102A(W) PA6, High Impact
Feature: Injection Molding, PA6, High ImpactApplication: H/Lamp Screw MountingCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical
|
|||
| Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1,-3 |
|
Gromax BFG30-FN00N1 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1,-3 |
|
Gromax BFG30-EN04B2 Nylon 6 36% Glass Filled (Conditioned)
Information provided by Gromax Enterprises Corp.
|
|||
| Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1,-3 |
|
Gromax BFG30-FH00B2 Nylon 6 30% Glass Filled (Conditioned)
Information provided by Gromax Enterprises Corp.
|
|||
| Melting Point | 220 °C | 428 °F | ISO 3146 |
|
Wellman Wellamid® 42LN2-N Nylon 6, General Purpose
All information provided by Wellman Engineered Resins.
|
|||
| Melting Point | 220 °C | 428 °F | ISO 3146 |
|
Wellman Wellamid® GF1685-WBK1 Nylon 6, 20% Glass Fiber Reinforced
All information provided by Wellman Engineered Resins.
|
|||
| Melting Point | 220 °C | 428 °F | ISO 3146 |
|
Chengdu Polyster H9275Y Thermoplastic Polyether-ester Elastomer (TPEE)
High modulus molding and injection grade. Contains improved color- stable antioxidants. Excellent heat-ageing resistance and toughness. Applications requiring high strength, high toughness and good ..
|
|||
| Melting Point | 220 °C | 428 °F | 10°C/min (DAM); ISO 11357-1/-3 |
|
DSM Akulon® K224-G6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1/-3 |
|
DSM Arnitel® PB582-H Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
|
|||
| Melting Point | 220 °C | 428 °F | ASTM D2133 |
|
Ensinger Tecast™ 6PA Natural Unfilled Cast Nylon 6 (PA6)
Tecast® 6PA Natural is an FDA-compliant grade used in applications requiring cast nylon but without any fillers.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of..
|
|||
| Melting Point | 220 °C | 428 °F | ASTM D2133 |
|
E-Polymers TEKAMID® TB120CR Fast Crystallinity PA6 Resin
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.T-series: Impact modified,..
|
|||
| Melting Point | 220 °C | 428 °F | ASTM D789 |
|
Adell AW-17 Nylon 66, 35% Glass Reinforced; Superior Finish
Data provided by Adell Plastics, Inc.
|
|||
| Melting Point | 220 °C | 428 °F | 10 K/min |
|
BASF Ultramid® HPN 9362 40% Mineral Filled PA6 (Dry)
Ultramid HPN 9362 is a 40% mineral reinforced, impact modified nylon 6 injection molding compound. It is one of the High Productivity Nylon series having improved surface appearance while reducing c..
|
|||
| Melting Point | 220 °C | 428 °F | ASTM and ISO test |
|
BASF Capron® 8232G HS BK-102 25% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron 8232G HS BK-102 is a pigmented black, heat stabilized, 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional..
|
|||
| Melting Point | 220 °C | 428 °F | ASTM and ISO test |
|
BASF Capron® 8253 Impact Modified Nylon 6 (Dry)
(discontinued **)
Capron 8253 is an unfilled type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Capron 8253 HS) and/or pigmented versions..
|
|||
| Melting Point | 220 °C | 428 °F | ASTM and ISO test |
|
BASF Capron® 8334G Impact Modified, 40% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron 8334G is a heat stabilized, 40% glass fiber reinforced polyamide 6 molding compound developed for applications requiring a high level of stiffness combined with excellent impact performance. ..
|
|||
| Melting Point | 220 °C | 428 °F | ASTM and ISO test |
|
BASF Capron® 8351 Impact Modified Nylon 6 (Dry)
(discontinued **)
Capron 8351 is a type 6 polyamide graft copolymer developed for injection molding applications requiring a high level of toughness combined with moderate flexibility and faster cycles. It is also ..
|
|||
| Melting Point | 220 °C | 428 °F | ASTM and ISO test |
|
BASF Capron® BG50XFI Impact Modified Nylon 6 (Dry)
(discontinued **)
Capron BG50XFI is an injection molding type 6 nylon graft copolymer with superior impact resistance and flow especially for thinner walled parts and long flow lengths. It is also available in natura..
|
|||
| Melting Point | 220 °C | 428 °F | ISO 3146/C2 |
|
Addiplast Addinyl B2 V30 Nylon 6, 30% Glass Filled
Glass fiber reinforced, high strengthInformation provided by Addiplast.
|
|||