Thermal Properties Metric English Comments
Melting Point 145 - 160 °C
293 - 320 °F
Peak; ASTM D3418
NatureWorks® Ingeo™ 8052D Foam Grade Biopolymer
Ingeo 8052D can be converted into an expanded foam sheet with use temperatures up to 77°F (25°C). This foam is lightweight, strong and suitable for packaging fresh meat and vegetables. In order to..
Melting Point 145 - 160 °C
293 - 320 °F
ASTM D3418
NatureWorks® Ingeo™ 6350D Fiber Grade PLA
NatureWorks PLA polymer 6350D is an amorphous thermoplastic spunbond-grade resin derived primarily from annually renewable resources. Available in pellet form, 6350D is designed for extrusion into s..
Melting Point 150 - 160 °C
302 - 320 °F
ASTM D3418
NatureWorks® Ingeo™ 6752D Spunbond Grade Biopolymer
Sheath polymer for spunbound uses. NatureWorks® PLA polymer 6752D, a NatureWorks LLC product, is a thermoplastic fiber-grade resin de-rived from annually renewable resources. Available in pellet f..
Melting Point 145 - 160 °C
293 - 320 °F
ASTM D3418
NatureWorks® Ingeo™ 7001D ISBM Bottle Grade Biopolymer
Ingeo biopolymer 7001D is a thermoplastic resin derived from annually renewable resources and is specifically designed for use in injection stretch blow molded (ISBM) bottle applications. Ingeo biop..
Melting Point 65.0 - 160 °C
149 - 320 °F
Average value: 116 °C Grade Count:52
Overview of materials for Anhydride-Modified Polyethylene
This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o..
Melting Point 150 - 160 °C
302 - 320 °F
3M Dyneon™ THV™ 400 Fluorothermoplastic  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.This unique, melt-processable, tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride (THV) terpolymer provides a unique combination of perf..
Melting Point 155 - 160 °C
311 - 320 °F
Hong Kun Group AO 1098 Antioxidant
Chemical Name: 3,3'-Bis(3,5-di-tert-butyl-4-hydroxyphenyl)-N,N'-hexamethylenedipropionamideCAS No. 23128-74-7All information provided by Hongkun Group
Melting Point 115 - 160 °C
239 - 320 °F
0.025" extruded film,
Huntsman IROGRAN® A 85 E 4719 TPU-Polyester
Introduction: IROGRAN A 85 E 4719 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a..
Melting Point 145 - 160 °C
293 - 320 °F
Huntsman/TMA
Huntsman IROGRAN® A 85 E 4993 FCM Polyester-Based TPU-Injection Extrusion Grade
IROGRAN A 85 E 4993 FCM is a thermoplastic polyester polyurethane for melt calendaring. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a specially..
Melting Point 115 - 160 °C
239 - 320 °F
0.025" extruded film,
Huntsman IROGRAN® A 85 E 5719 FCM TPU-Polyester
Introduction: IROGRAN A 85 E 5719 FCM is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offe..
Melting Point 145 - 160 °C
293 - 320 °F
ISO 3146-C
FKuR Kunststoff Bio-Flex® F 2201 CL Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..
Melting Point 140 - 160 °C
284 - 320 °F
ISO 3146-C
FKuR Kunststoff Bio-Flex® S 5630 Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..
Melting Point 150 - 160 °C
302 - 320 °F
ISO 3146-C
FKuR Kunststoff Fibrolon® F 8530 Biodegradable Wood-Plastic Compound, Fiber Reinforced
FIBROLON® are fiber reinforced compounds. Depending on specific customer requirements either a biodegradable polymer or a polyolefin can be used as the polymeric matrix. With the brand name of F..
Melting Point 122 - 160 °C
252 - 320 °F
Indium Corp. Indalloy 93 Bismuth-Lead Solder Alloy
Information Provided by Indium Corporation
Melting Point 120 - 160 °C
248 - 320 °F
LG Chemical SEETEC T3410 Polypropylene Random Terpolymer
Features: Seetec T3410 is a polypropylene-ethylene-butene random terpolymer designed for the production of Transparent Film and Expandable PP for low seal temperature and high impact strength. It of..
Melting Point 150 - 160 °C
302 - 320 °F
MQSA 111
Lubrizol Advanced Materials PEARLCOAT® 168K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 168K is a polyether-based TPU, supplied in form of translucent, colorless pellets, offering adequate hardness, excellent low-temperature flexibility and very good hydrolysis resistance..
Melting Point 156 - 160 °C
313 - 320 °F
DSC
Solvay Specialty Polymers Hylar® 5000 Polyvinylidene Fluoride (PVDF)
Hylar® 5000 is a crystalline high molecular weight powder form of polyvinylidene fluoride (PVDF) specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically ..
Melting Point 156 - 160 °C
313 - 320 °F
DSC
Solvay Specialty Polymers Hylar® Latex 932 Polyvinylidene Fluoride (PVDF)
Hylar® Latex 932 is a stabilized aqueous dispersion that contains approximately 22% by weight of a high molecular weight PVDF polymer (polyvinylidene fluoride) of medium crystallinity. The disper..
Melting Point 100 - 160 °C
212 - 320 °F
Sibur AGG-G/B Atactic Polypropylene
For preparation of polymer, bitumen-polymer and polymer-mineral mastics. Individual melts and compositions used for anti-corrosion covers for underground piping, different building structures, stru..
Melting Point 100 - 160 °C
212 - 320 °F
Sibur APP-B Atactic Polypropylene
For preparation of polymer, bitumen-polymer and polymer-mineral mastics. Individual melts and compositions used for anti-corrosion covers for underground piping, different building structures, stru..
Melting Point 156 - 160 °C
313 - 320 °F
ISO 3146
Borealis Borflow™ HL508FB Polypropylene Homopolymer
Borflow HL508FB is a polypropylene homopolymer grade intended for fiber applications characterized by narrow molecular weight distribution, controlled rheology, easy processability, optimal product ..
Melting Point 156 - 160 °C
313 - 320 °F
ISO 3146
Borealis Borflow™ HL512FB Polypropylene Homopolymer
Borflow HL512FB is a polypropylene homopolymer grade intended for fiber applications characterized by narrow molecular weight distribution, controlled rheology, easy processability, optimal product ..
Melting Point 150 - 160 °C
302 - 320 °F
DSC
EMS-Griltech Griltex® D 1377E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melting Point 155 - 160 °C
311 - 320 °F
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Melting Point 155 - 160 °C
311 - 320 °F
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Melting Point 155 - 160 °C
311 - 320 °F
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Melting Point 156 - 160 °C
313 - 320 °F
ASTM D3418
Solvay Specialty Polymers Hylar® 5000 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Hylar 5000 is a crystalline high molecular weight powder form of polyvinylidene fluoride specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically strong and ..
Melting Point 155 - 160 °C
311 - 320 °F
Arkema Group KYNAR FLEX® 2850 PC Polyvinylidene Fluoride Spray Coating Powder
Electrostatic sprayInformation provided by Arkema Inc.
Melting Point 155 - 160 °C
311 - 320 °F
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Melting Point 155 - 160 °C
311 - 320 °F
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Copyright © lookpolymers.com All Rights Reserved