Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 324 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Melting Point 162 °C
324 °F
Private Lab
Polymer Industries Densetec PP Copolymer Sheet
Polymer Industries’ Densetec Copolymer Propylene differs from the Densetec Homopolymer Polypropylene by virtue of an additional monomer in the product, thus making it a copolymer material. This is ..
Melting Point 162 - 180 °C
324 - 356 °F
Average value: 173 °C Grade Count:3
Overview of materials for Polycarbonate-Urethane
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate-Urethane". Each property range of values reported is minimum and maximum values of appropr..
Melting Point 162 - 185 °C
324 - 365 °F
Average value: 167 °C Grade Count:19
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
Melting Point 162 °C
324 °F
DSC; ISO 11357-1,-3
Inno-Comp INNOPOL® CS 1-3120 B DEL 20% Talc Filled Polypropylene Homopolymer
INNOPOL® CS 1-3120 B DEL is developed for producing injection molded automotive components.All information provided by INNO-COMP.
Melting Point 162 - 168 °C
324 - 334 °F
Sheath Melt Point; LCL-PR29
Intercontinental Polymers 1180 Bicomponent PP/PET Fiber Type - 3 Denier X 1.5 Inches
40/60 PP Sheath/PET Core. Luster: Semi-Dull. Finish: Hydrophilic.Applications of bicomponent polyester fiber: Absorbent products, hygiene products, non-wovens, filtration, sliver knit, microdenier..
Melting Point 162 °C
324 °F
Techmer ES Elastoblend® POM CO IM MB
Availability: North AmericaForms: PelletsAdditive: Impact Modifier Features: Impact Modified and CopolymerInformation provided by TP Composites, Inc.
Melting Point 162 - 168 °C
324 - 334 °F
DSC
Solvay Specialty Polymers Ajediumâ„¢ PVDF 9009 Polyvinylidene Fluoride (PVDF)
Solef® 9009 PVDF homopolymer is a semi-crystalline fluoropolymer. Solef® film is chemically inert to most acids, aliphatic and aromatic organic compounds, chlorinated solvents and alcohols.Fea..
Melting Point 162 - 168 °C
324 - 334 °F
DSC
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF)
Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 53...
Melting Point 162 °C
324 °F
Techmer ES Luriblend® POM HO TL20 BN042 Acetal
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated and HomopolymerAppearance: Brown, Natural Color and RedInformation provided by TP Composites, Inc.
Melting Point 162 - 165 °C
324 - 329 °F
ISO 3146
Borealis Daploy™ WF420HMS High Melt Strength Polypropylene for Extrusion Coating
Daploy WF420HMS resin is a propylene-based, structurally isomeric polymer, which combines significantly increased melt strength with largely drawability of the polymer melt. Thus, the material is g..
Melting Point 162 - 165 °C
324 - 329 °F
DSC; ISO 3146
Borealis HB205TF Polypropylene
HB205TF is a low melt flow rate polypropylene homopolymer intended for extrusion, calendering and thermoforming. Its very good organoleptic properties allows this grade to be used with any master b..
Melting Point 162 - 166 °C
324 - 331 °F
DSC; ISO 3146
Borealis HC600TF Polypropylene
HC600TF is a polypropylene homopolymer intended for thermoformed packaging applications. Its very good organoleptic properties allows this grade to be used with any masterbatch without discoloring ..
Melting Point 162 - 166 °C
324 - 331 °F
DSC; ISO 3146
Borealis HD204CF Polypropylene
HD204CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: HD204CF is recommended for medical applications, inner layer in co extru..
Melting Point 162 - 166 °C
324 - 331 °F
DSC; ISO 3146
Borealis HD244CF Polypropylene
HD244CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: food packaging, lamination films, stationery folders, multi layer co-extr..
Melting Point 162 - 166 °C
324 - 331 °F
DSC; ISO 3146
Borealis HD621CF Polypropylene
HD621CF is a polypropylene homopolymer This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: food packaging, lamination films, statio..
Melting Point 162 °C
324 °F
ISO 3146
Total PPH 3150 Polypropylene, Homopolymer
Polypropylene PPH 3150 is a modified homopolymer polypropylene with a Melt Flow index of 2 g/10 min.Polypropylene PPH 3150 is intended for the production at very high speed of flat bioriented films ..
Melting Point 162 °C
324 °F
Peak; ExxonMobil Method
ExxonMobil EXXELOR™ PO 1020 Maleic anhydride functionalized polypropylene
Product Description: Exxelor PO 1020 polymer resin is a high performance maleic anhydride fuctionalized homopolypropylene produced by reactive extrusion. It has been primarily designed to add polari..
Melting Point 162 °C
324 °F
DSC; Dow Method
Dow C702-20 Polypropylene Impact Copolymer Resin
OverviewHigh impactComplies with: U.S. FDA FCN 843, Canadian HPFB No ObjectionDOW C702-20 Polypropylene Resin is intended for use in injection molded applications requiring high impact. It is parti..
Melting Point 162 °C
324 °F
DSC; Dow Method
Dow H700-12 Polypropylene Homopolymer Resin
Complies withU.S. FDA 21 CFR 177.1520 (c) 1.1FDA-DMFUnderwriters Laboratories Inc.Europe EU-Directive 2002/72/ECLondon Metal Exchange - Part 6B Rules - PolypropyleneCanadian HPFB No ObjectionDOW H70..
Melting Point 162 °C
324 °F
ISO 3146
Eurostar Starpylen HU 70E4 ECR
Starpylen HU 70E4 ECR is a Renewable Calcium Carbonate (oyster shell) Masterbatch in a PP carrier. Engineered to reduce carbon footprint in mineral filled compound.Information provided by Eurostar.
Melting Point 162 °C
324 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET  (Unverified Data**)
Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various..
Melting Point 162 °C
324 °F
ASTM D3418
E-Polymers EFLEX® M400 PP Homopolymer
M-series: E-FLEX M series resins are a maleic anhydride grafted (MAH) polymer concentrate designed as synthetic rubber and polyolefin manufactured by E-Polymers. It offers excellent adhesion to nyl..
Melting Point 162 - 167 °C
324 - 333 °F
Addcomp PRIEX® Ionomer 40101 PP homopolymer
Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t..
Melting Point 162 °C
324 °F
Techmer ES Luriblend® POM CO GF5 TL5 5% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 5% Filler by WeightAdditive: PTFE Lubricant(5%)Features: Lubricated and CopolymerInformation provided by TP Composites, In..
Melting Point 162 °C
324 °F
Techmer ES Luriblend® POM HO TL20 BK Acetal
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated and HomopolymerAppearance: BlackInformation provided by TP Composites, Inc.
Melting Point 162 - 168 °C
324 - 334 °F
ASTM D3418
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers.
Melting Point 162 - 168 °C
324 - 334 °F
ASTM D3418
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)  (discontinued **)
Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers.
Melting Point 162 - 167 °C
324 - 333 °F
Average value: 166 °C Grade Count:11
Overview of materials for Acetal Copolymer, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of ..
Melting Point 162 - 180 °C
324 - 356 °F
Average value: 172 °C Grade Count:11
Overview of materials for Acetal Homopolymer, PTFE-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o..
Melting Point 162 - 170 °C
324 - 338 °F
Average value: 166 °C Grade Count:38
Overview of materials for Acetal Copolymer, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values..