Polymer Property : UL RTI, Mechanical without Impact = 221 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746
PolyOne Maxxam™ FR PP 401 Polypropylene, Unspecified (PP, Unspecified)
Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V..
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS
PC+ABS, excellent impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components.
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Europe-Africa-Middle East)
CYCOLOY C1200 is a PC+ABS blend developed to serve extremely demanding applications in a variety of markets while maintaining good processing properties. The combination of superior heat resistance ..
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS (Asia Pacific)
PC+ABS, excellent flow/impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components.
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Asia Pacific)
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Europe-Africa-Middle East)
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
UL RTI, Mechanical without Impact 105 °C
221 °F
Ul746B
Parker Chomerics PREMIER™ A220-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
UL RTI, Mechanical without Impact 105 °C
221 °F
Ul746B
Parker Chomerics PREMIER™ A240-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS (Europe-Africa-Middle East)
CYCOLOY C1200HF is the improved version of CYCOLOY C1200 and has been developed to provide enhanced productivity and surface appearance for
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS (Europe-Africa-Middle East)
CYCOLOY FXC810SK is a multi purpose PC+ABS injection moulding grade, providing a favourable balance of engineering properties. CYCOLOY FXC810SK is suitable for those applications that require sparkl..
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics Cycoloy® FXC810SL PC+ABS (Europe-Africa-Middle East)
CYCOLOY FXC810SL is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require sparkle colour effects with lowered RFI inhibitor. Colour package may effect perform..
UL RTI, Mechanical without Impact 105 °C
221 °F
UL746B
Idemitsu Kosan Xarec® WA 550 SPS, 30% Glass Filled
Crystalline Polymer, Glass Filled. Used in Automotive and Industrial applications
UL RTI, Mechanical without Impact 105 °C
221 °F
Lucent Polymers PC-FR0 Polycarbonate, Flame Resistant
UV Stable/Weatherable, f1 RatedMelt Flow Adjustable for Application UL File Number: E213588Information provided by Lucent Polymers, Inc.
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics ULTEM 2110EPR PEI (Asia Pacific)
10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics ULTEM 2212EPR PEI
20% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA lising.
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics ULTEM 2212EPR PEI (Asia Pacific)
20% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA lising.
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics Ultem 2313 PEI (Asia Pacific)
30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific regi..
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics ULTEM 2410R PEI (Europe-Africa-Middle East)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing.
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics ULTEM CRS5201 PEI
20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing.
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics Ultem CRS5211 PEI
20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing.Th..
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics ULTEM CRS5311 PEI (Asia Pacific)
30% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing.
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics ULTEM CRS5311 PEI (Europe-Africa-Middle East)
30% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS compliant. UL94 V0 and 5VA li..
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI
LNP* Stat-kon* Ultem_UC1200 is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications.
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics NORYL N300X PPE+PS (Asia Pacific)
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications.
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics Valox® 365 PET
Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031".This data was supplied by SABIC-IP for the Americas region.
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics Valox® 745 PBT (Asia Pacific)
30% mineral reinforced polyester improved toughness and low warpage. Typical applications are telephone ringer frames and card racks.
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746
Styron EMERGEâ„¢ 4410-18 MFR Polycarbonate
EMERGEâ„¢ PC 4410-18 advanced resin is a high impact polycarbonate resin designed for Information Technology Equipment and Injection Molding Applications.Information provided by DowThis product l..
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics NORYL 731 PPE+PS
PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi..
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
SABIC Innovative Plastics Noryl 731H PPE+PS
High gloss, general purpose grade. 130C (266F) DTUL. UL 94 HB rated. For multiple plugs, wine filter plates, etc.This data was supplied by SABIC-IP for the Americas region.