Polymer Property : Glow Wire Test = 800 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS (Asia Pacific)
Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes..
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che..
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1...
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS
Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc..
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer
Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3..
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer (Asia Pacific)
Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3..
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer (Europe-Africa-Middle East)
Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3..
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer
ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system.
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer
ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system.
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics LNP KONDUIT PX11313 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 FR compounding
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS (Asia Pacific)
Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che..
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo..
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics Lexan® 945U PC
Lexan* 945U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio..
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL PX9406K PPE+HIPS (Asia Pacific)
NORYL* PX9406K resin may be suitable for consumer electronics applications. Flame retardant used is non-halogenated. UL94 V0 at 1.5 mm, 5VB at 2 mm, and 5VA at 2.5 mm. RTI (impact) = 105 C
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL PX9406K PPE+HIPS (Asia Pacific)
NORYL* PX9406K resin may be suitable for consumer electronics applications. Flame retardant used is non-halogenated. UL94 V0 at 1.5 mm, 5VB at 2 mm, and 5VA at 2.5 mm. RTI (impact) = 105 C
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL SE1GFN1 PPE+HIPS (Europe-Africa-Middle East)
Noryl* SE1GFN1 is a 10% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non..
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL WCA875 PPE-TPE (Europe-Africa-Middle East)
Non-halogenated flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Excellent flame retardant performance with balanced t..
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL WCP821 PPE-TPE
Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain ..
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Asia Pacific)
Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain ..
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Europe-Africa-Middle East)
Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain ..
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Asia Pacific)
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS
Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 ..
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS
Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to..
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to..
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS
Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng..
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL WCD851 PPE-TPE (Asia Pacific)
Flexible, strong flame-retardant, halogen-free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame retardant performance capable of meeting UL VW-..
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Europe-Africa-Middle East)
Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be..
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Europe-Africa-Middle East)
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East)
Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances.
Glow Wire Test 800 °C
1470 °F
Glow Wire Flammability Index; IEC 60695-2-12
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA)  (Unverified Data**)
Amodel HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a broad..