| Category | Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Cycoloy® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Europe-Africa-Middle East).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.19 g/cc | 1.19 g/cc | ASTM D792 |
| Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.100 % | 0.100 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.20 % | 0.20 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 18 g/10 min @Load 2.16 kg, Temperature 260 °C |
18 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
| Melt Index of Compound | 15 g/10 min @Load 2.16 kg, Temperature 260 °C |
15 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 50.0 MPa | 7250 psi | 50 mm/min; ISO 527 |
| 58.0 MPa | 8410 psi | Type I, 50 mm/min; ASTM D638 | |
| Tensile Strength, Yield | 65.0 MPa | 9430 psi | Type I, 50 mm/min; ASTM D638 |
| 65.0 MPa | 9430 psi | 50 mm/min; ISO 527 | |
| Elongation at Break | 90 % | 90 % | 50 mm/min; ISO 527 |
| 100 % | 100 % | Type I, 50 mm/min; ASTM D638 | |
| Elongation at Yield | 4.0 % | 4.0 % | 50 mm/min; ISO 527 |
| 4.1 % | 4.1 % | Type I, 50 mm/min; ASTM D638 | |
| Tensile Modulus | 2.60 GPa | 377 ksi | 5 mm/min; ASTM D638 |
| 2.60 GPa | 377 ksi | 1 mm/min; ISO 527 | |
| Flexural Yield Strength | 96.0 MPa | 13900 psi | 2 mm/min; ISO 178 |
| 104 MPa | 15100 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Flexural Modulus | 2.50 GPa | 363 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 2.50 GPa | 363 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
| 1.75 J/cm @Temperature -30.0 °C |
3.28 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*3; ISO 180/1A |
| 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1A | |
| 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
| 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A | |
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
| 2.20 J/cm² | 10.5 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA | |
| 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA | |
| Dart Drop, Total Energy | 65.0 J @Temperature 23.0 °C |
47.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 75.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
41.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 |
| Deflection Temperature at 0.46 MPa (66 psi) | 100 °C @Thickness 3.20 mm |
212 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 93.0 °C | 199 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 89.0 °C @Thickness 3.20 mm |
192 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| 99.0 °C @Thickness 6.40 mm |
210 °F @Thickness 0.252 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 110 °C | 230 °F | Rate B/50; ASTM D1525 |
| 110 °C | 230 °F | Rate B/50; ISO 306 | |
| 113 °C | 235 °F | Rate B/120; ISO 306 | |
| UL RTI, Electrical | 90.0 °C | 194 °F | UL 746B |
| UL RTI, Mechanical with Impact | 90.0 °C | 194 °F | UL 746B |
| UL RTI, Mechanical without Impact | 90.0 °C | 194 °F | UL 746B |
| Flammability, UL94 | V-1 @Thickness 0.600 mm |
V-1 @Thickness 0.0236 in |
UL 94 |
| V-0 @Thickness 0.750 mm |
V-0 @Thickness 0.0295 in |
UL 94 | |
| 5VB @Thickness 1.50 mm |
5VB @Thickness 0.0591 in |
UL 94 | |
| 5VA @Thickness 3.00 mm |
5VA @Thickness 0.118 in |
UL 94 | |
| Oxygen Index | 34 % | 34 % | ISO 4589 |
| Glow Wire Test | 775 °C | 1430 °F | IEC 60695-2-13 |
| 775 °C | 1430 °F | IEC 60695-2-13 | |
| 775 °C | 1430 °F | IEC 60695-2-13 | |
| 800 °C | 1470 °F | IEC 60695-2-13 | |
| 825 °C | 1520 °F | IEC 60695-2-13 | |
| 960 °C @Thickness 0.750 mm |
1760 °F @Thickness 0.0295 in |
IEC 60695-2-12 | |
| 960 °C @Thickness 0.750 mm |
1760 °F @Thickness 0.0295 in |
IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ROA; IEC 60093 |
| Dielectric Strength | 17.0 kV/mm @Thickness 3.20 mm |
432 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
| 25.0 kV/mm @Thickness 1.60 mm |
635 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 | |
| 35.0 kV/mm @Thickness 0.800 mm |
889 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 | |
| Comparative Tracking Index | 175 - 250 V | 175 - 250 V | UL 746A |
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
| High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ball Pressure Test, 75°C +/- 2°C | Pass | IEC 60695-10-2 |