Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 284 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 120 - 140 °C
248 - 284 °F
Injection; ISO 75-A
Raschig Group 3536 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed..
Deflection Temperature at 1.8 MPa (264 psi) 93.0 - 140 °C
199 - 284 °F
Average value: 110 °C Grade Count:7
Overview of materials for Nylon, Amorphous Transparent Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value..
Deflection Temperature at 1.8 MPa (264 psi) 100 - 140 °C
212 - 284 °F
Average value: 114 °C Grade Count:9
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend". Each property range of values reported is minimum and ma..