Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 51.0 - 55.0 °C
124 - 131 °F
ASTM D648
Proto3000 Accura® 25 Plastic Stereolithography (SLA) Prototyping Polymer
Description: A high stiffness engineered nanocomposite that opens new applications for stereolithography users. Features: Look and feel of molded polypropyleneOutstanding feature resolution and accu..
Deflection Temperature at 1.8 MPa (264 psi) 51.0 - 55.0 °C
124 - 131 °F
ASTM D648-07
Proto3000 Objet Digital Materials™ RGD5160-DM ABS-like Prototyping Polymer
Objet ABS-like Digital Material made of Object RGD515 & Objet RGD535Digital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to..
Deflection Temperature at 1.8 MPa (264 psi) 40.0 - 55.0 °C
104 - 131 °F
ASTM D648
Arkema Group Kynar Flex® 2900 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Deflection Temperature at 1.8 MPa (264 psi) 45.0 - 55.0 °C
113 - 131 °F
Average value: 49.8 °C Grade Count:4
Overview of materials for Nylon 11, Cable Sheathing Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Cable Sheathing Grade". Each property range of values reported is minimum and maximum values o..
Deflection Temperature at 1.8 MPa (264 psi) 36.0 - 55.0 °C
96.8 - 131 °F
Average value: 43.1 °C Grade Count:7
Overview of materials for Nylon 11, Flexible Tubing Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Flexible Tubing Grade". Each property range of values reported is minimum and maximum values o..
Deflection Temperature at 1.8 MPa (264 psi) 40.0 - 55.0 °C
104 - 131 °F
ASTM D648
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Deflection Temperature at 1.8 MPa (264 psi) 40.0 - 55.0 °C
104 - 131 °F
ASTM D648
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s..
Deflection Temperature at 1.8 MPa (264 psi) 38.0 - 55.0 °C
100 - 131 °F
ASTM D648
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Deflection Temperature at 1.8 MPa (264 psi) 38.0 - 55.0 °C
100 - 131 °F
ASTM D648
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Deflection Temperature at 1.8 MPa (264 psi) 38.0 - 55.0 °C
100 - 131 °F
ASTM D648
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Deflection Temperature at 1.8 MPa (264 psi) 40.0 - 55.0 °C
104 - 131 °F
ASTM D648
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
Deflection Temperature at 1.8 MPa (264 psi) 51.0 - 55.0 °C
124 - 131 °F
ASTM D648
3D Systems Accura® 25 Plastic for SLA® Systems
For use with solid-state stereolithography (SLA®) systems.ApplicationsFunctional components for assemblies and mock-ups for:Automotive styling parts — trim, fascia, and other componentsConsumer el..
Deflection Temperature at 1.8 MPa (264 psi) 40.0 - 55.0 °C
104 - 131 °F
Average value: 49.8 °C Grade Count:24
Overview of materials for Nylon 11, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Deflection Temperature at 1.8 MPa (264 psi) 40.0 - 55.0 °C
104 - 131 °F
ASTM D648
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Deflection Temperature at 1.8 MPa (264 psi) 38.0 - 55.0 °C
100 - 131 °F
ASTM D648
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Deflection Temperature at 1.8 MPa (264 psi) 38.0 - 55.0 °C
100 - 131 °F
ASTM D648
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Copyright © lookpolymers.com All Rights Reserved