Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 0.144 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.144 W/m-K
1.00 BTU-in/hr-ft²-°F
ASTM C177
Quantum PEI - Ultem®
Information provided by Quantum Advanced Engineering Plastics
Thermal Conductivity >= 0.144 W/m-K
>= 1.00 BTU-in/hr-ft²-°F
ASTM C177
PolyOne Edgetek® SY-03CF/000 Polystyrene - High Impact (HIPS), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedUL 94 HB (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation.
Thermal Conductivity 0.144 - 0.180 W/m-K
1.00 - 1.25 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group Kynar Flex® 2900 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Thermal Conductivity 0.144 - 0.180 W/m-K
1.00 - 1.25 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group Kynar Flex® 2950 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Thermal Conductivity 0.144 - 0.180 W/m-K
1.00 - 1.25 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group Kynar Flex® 3120 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Thermal Conductivity 0.144 - 0.180 W/m-K
1.00 - 1.25 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR FLEX® 2500-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Highest flexibility. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical st..
Thermal Conductivity 0.144 - 0.180 W/m-K
1.00 - 1.25 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Thermal Conductivity 0.144 - 0.180 W/m-K
1.00 - 1.25 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s..
Thermal Conductivity 0.144 - 0.180 W/m-K
1.00 - 1.25 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Thermal Conductivity 0.144 - 0.180 W/m-K
1.00 - 1.25 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Thermal Conductivity 0.144 - 0.180 W/m-K
1.00 - 1.25 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Thermal Conductivity 0.144 - 0.180 W/m-K
1.00 - 1.25 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
Thermal Conductivity 0.144 - 0.180 W/m-K
1.00 - 1.25 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
Thermal Conductivity 0.144 - 0.180 W/m-K
1.00 - 1.25 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
Thermal Conductivity 0.144 - 0.180 W/m-K
1.00 - 1.25 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Thermal Conductivity 0.144 - 0.180 W/m-K
1.00 - 1.25 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Thermal Conductivity 0.144 - 0.180 W/m-K
1.00 - 1.25 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Thermal Conductivity 0.144 - 0.180 W/m-K
1.00 - 1.25 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low..
Thermal Conductivity 0.144 - 0.180 W/m-K
1.00 - 1.25 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Thermal Conductivity 0.144 - 0.180 W/m-K
1.00 - 1.25 BTU-in/hr-ft²-°F
ASTM D433
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Copyright © lookpolymers.com All Rights Reserved