Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.144 - 0.180 W/m-K | 1.00 - 1.25 BTU-in/hr-ft²-°F | ASTM D433 |
Arkema Group Kynar Flex® 2900 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Thermal Conductivity | 0.144 - 0.180 W/m-K | 1.00 - 1.25 BTU-in/hr-ft²-°F | ASTM D433 |
Arkema Group Kynar Flex® 2950 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Thermal Conductivity | 0.144 - 0.180 W/m-K | 1.00 - 1.25 BTU-in/hr-ft²-°F | ASTM D433 |
Arkema Group Kynar Flex® 3120 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Thermal Conductivity | 0.144 - 0.180 W/m-K | 1.00 - 1.25 BTU-in/hr-ft²-°F | ASTM D433 |
Arkema Group KYNAR FLEX® 2500-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Highest flexibility. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical st.. |
|||
Thermal Conductivity | 0.144 - 0.180 W/m-K | 1.00 - 1.25 BTU-in/hr-ft²-°F | ASTM D433 |
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
Thermal Conductivity | 0.144 - 0.180 W/m-K | 1.00 - 1.25 BTU-in/hr-ft²-°F | ASTM D433 |
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s.. |
|||
Thermal Conductivity | 0.144 - 0.180 W/m-K | 1.00 - 1.25 BTU-in/hr-ft²-°F | ASTM D433 |
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Thermal Conductivity | 0.144 - 0.180 W/m-K | 1.00 - 1.25 BTU-in/hr-ft²-°F | ASTM D433 |
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Thermal Conductivity | 0.144 - 0.180 W/m-K | 1.00 - 1.25 BTU-in/hr-ft²-°F | ASTM D433 |
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Thermal Conductivity | 0.144 - 0.180 W/m-K | 1.00 - 1.25 BTU-in/hr-ft²-°F | ASTM D433 |
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Thermal Conductivity | 0.144 - 0.180 W/m-K | 1.00 - 1.25 BTU-in/hr-ft²-°F | ASTM D433 |
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Thermal Conductivity | 0.144 - 0.180 W/m-K | 1.00 - 1.25 BTU-in/hr-ft²-°F | ASTM D433 |
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Thermal Conductivity | 0.144 - 0.180 W/m-K | 1.00 - 1.25 BTU-in/hr-ft²-°F | ASTM D433 |
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Thermal Conductivity | 0.144 - 0.180 W/m-K | 1.00 - 1.25 BTU-in/hr-ft²-°F | ASTM D433 |
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Thermal Conductivity | 0.0300 - 0.180 W/m-K | 0.208 - 1.25 BTU-in/hr-ft²-°F | Average value: 0.0389 W/m-K Grade Count:9 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Thermal Conductivity | 0.144 - 0.180 W/m-K | 1.00 - 1.25 BTU-in/hr-ft²-°F | ASTM D433 |
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Thermal Conductivity | 0.144 - 0.180 W/m-K | 1.00 - 1.25 BTU-in/hr-ft²-°F | ASTM D433 |
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
Thermal Conductivity | 0.144 - 0.180 W/m-K | 1.00 - 1.25 BTU-in/hr-ft²-°F | ASTM D433 |
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Thermal Conductivity | 0.144 - 0.180 W/m-K | 1.00 - 1.25 BTU-in/hr-ft²-°F | ASTM D433 |
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |