Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 135 °C | 275 °F | short period, no load |
Omnia Plastica PC Polycarbonate This amorphous polymer is commonly used for its high shock resistance even at low temperature. It is not a material recommended for mechanical applications, even if its dimensional stability does ma.. |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | |
NextGen Adhesives M907-20 Medical Grade Epoxy Adhesive Description: NGAC M907-20 is a medium viscosity adhesive system that is specifically formulated for medical device assembly applications.Advantages and Applications: Uses include laminating, bonding.. |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | Continuous (GTP 50% Tensile); IEC 60216 |
PolyOne Bergadur™ PB40 G15 U SO1 BK Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | Continuous (GTP 50% Tensile); IEC 60216 |
PolyOne Bergadur™ PB40 G15 UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 135 - 250 °C | 275 - 482 °F | Average value: 186 °C Grade Count:6 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | |
Lehmann & Voss LUVOCOM® 1t-7370 Polyamide 6/6T, with carbon fiber, toughness-modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | |
Lehmann & Voss LUVOCOM® 21-7976 Polyamide 6/6T, with glass fiber and PTFE, 8-mm-granulate Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | |
Greene Tweed WR™ FP100 Polyketone, Reinforced Greene Tweed’s WR® FP100, a reinforced compression-molded polyketone, offers excellent wear resistance with FDA compliance. The typical properties and physical characteristics of WR FP100 m.. |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | |
LATI Later 4 G/30 PBT, 30% Glass Fiber Reinforced Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | |
LATI Later 4 G/30-V0 PBT, 30% Glass Fiber Reinforced, Flame Retardant Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am.. |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | |
Trelleborg P650 Epichlorohydrin There are three types of epichlorohydrin:1. Homopolymers of epichlorohydrin. Designated CO.2. Chopolymers of epichlorohydrin and etylene oxide. Designated ECO.Terpolymers of epichlorohydrin, etylene.. |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | Wet Service (water) |
Chesterton ARC S7 High Temperature & Chemical Resistant Novolac Vinyl Ester Coating Description: ARC S7 is a low VOC, epoxy novolac vinyl ester based coating intended for high temperature exposures in chemically aggressive applications where the risk for thermal cycling may be pres.. |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | |
ExxonMobil Santoprene® 121-58W175 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for .. |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | |
ExxonMobil Santoprene® 121-67W175 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for .. |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | |
ExxonMobil Santoprene® 201-73 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | few hours; VDE 0304/P2-1, IEC 216 |
EPICHEM Epilon FR-PC V0 Polycarbonate Characteristics: self-extinguishing V0 at 1,6 mm |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | at 50% loss of tensile strength after 20000h; IEC 216-1 |
BASF Ultradur B 4300 G4 20% Glass Filled PBT Ultradur B4300 G4 is an easy flowing injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | for 50% loss of tensile strength after 20000hr |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Dry) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | for 50% loss of tensile strength after 20000hr |
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Conditioned) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | for 50% loss of tensile strength after 20000hr |
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Conditioned) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | for 50% loss of tensile strength after 20000hr |
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Dry) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | for 50% loss of tensile strength after 20000hr |
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Conditioned) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | for 50% loss of tensile strength after 20000hr |
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Dry) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | at 50% loss of tensile strength after 5000h; IEC 216-1 |
BASF Ultradur® B 4406 PBT Description: Is a PBT, flame-retardant injection-molding grades, unreinforced for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and lighting compo.. |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | |
3M Scotch® FP-301VW Heat Shrink Tubing Scotch® Heat Shrink Tubing FP-301VW has the same outstanding balance of electrical, physical and chemical properties as FP-301 tubing, and is specially engineered for excellent flame resistance. FP.. |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | for 50% loss of tensile strength after 5000hr |
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Conditioned) Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el.. |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | for 50% loss of tensile strength after 20000hr |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | |
ExxonMobil Santoprene® 221-87 Thermoplastic Elastomer
(discontinued **) A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | |
ExxonMobil Santoprene® 101-87 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Maximum Service Temperature, Air | 135 °C | 275 °F | |
Resinlab® CYNERGY CA6903 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |