Polymer Property : Maximum Service Temperature, Air = 284 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 140 °C
284 °F
Continuous; FRISETTA Test Method
Nilit FRIANYL A63 HH-SG-GV 2020 Nylon 6.6 for injection molding, 20% mineral filled, 20% glass fiber reinforced
Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Maximum Service Temperature, Air 140 - 150 °C
284 - 302 °F
Short Term
Kolon Kocetal® TC704 Reinforced Grade Acetal Copolymer  (Unverified Data**)
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..
Maximum Service Temperature, Air 140 - 150 °C
284 - 302 °F
Short Term
Kolon Kocetal® EC701 Modified Grade Acetal Copolymer  (discontinued **)
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..
Maximum Service Temperature, Air 140 - 150 °C
284 - 302 °F
Short Term
Kolon Kocetal® DP301 Modified Grade Acetal Copolymer  (discontinued **)
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..
Maximum Service Temperature, Air 140 - 150 °C
284 - 302 °F
Short Term
Kolon Kocetal® VT701 Modified Grade Acetal Copolymer  (discontinued **)
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..
Maximum Service Temperature, Air 140 °C
284 °F
short term
Lehmann & Voss LUVOCOM® 6-8159 Polyamide 12, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Especially suitable at dynamic stress situations.Electrically conductive, s..
Maximum Service Temperature, Air 140 °C
284 °F
short term
Lehmann & Voss LUVOCOM® 6-8438-1 Polyamide 12, with glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Suitable for discharging of statically generated electricity.Dynamic stressed parts.Low waterab..
Maximum Service Temperature, Air 140 °C
284 °F
Intermittent
Global EPP POM C Acetal Copolymer
Polyacetals are highly crystalline thermoplastics, characterised by their high mechanical strength, rigidity and impact resistance. Acetal absorbs very little moisture, enabling the product to maint..
Maximum Service Temperature, Air 140 °C
284 °F
short term
Lehmann & Voss LUVOCOM® 1-0867 Polyamide 66, with aramid reinforcement and PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinka..
Maximum Service Temperature, Air 140 °C
284 °F
short term
Lehmann & Voss LUVOCOM® NSB 90 BK Polyamide 66, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Maximum Service Temperature, Air 140 °C
284 °F
short term
Lehmann & Voss LUVOTECH® GS 58 Polyamide 66, with glass fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Maximum Service Temperature, Air 140 °C
284 °F
LATI Laramid CE/60 PPA, 60% Mineral Reinforced
Semi-aromatic polyamide (PPA) based compound. Mineral filler. High dimensional stability. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Maximum Service Temperature, Air 140 °C
284 °F
Short peaks operation
Polyram PlusTek PA303G6BK16 Nylon 6.6, 30% Glass Fiber reinforced, Heat Stabilized, Hydrolysis Resistant
30% Glass fiber reinforced, heat stabilized, hydrolysis resistant, improved surface finish Nylon 6.6. Approved and listed by W.R.A.S.Information provided by Polyram.
Maximum Service Temperature, Air 140 °C
284 °F
Tra-Con Tra-Bond FDA25 Food and Drug Application Epoxy Adhesive
TRA-BOND FDA-25 is a medium viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Admi..
Maximum Service Temperature, Air 140 °C
284 °F
Tra-Con Tra-Bond 2105 Clear Rigid, Medium Viscosity Epoxy Adhesive
TRA-BOND 2105 is a clear, medium viscosity epoxy adhesive which contains no solvents or other additives which can be harmful to the environment or to its users. It has excellent adhesion to glass, c..
Maximum Service Temperature, Air 140 °C
284 °F
Elastron® V TPV Elastomer
Characteristicswide hardness rangedoes not require vulcanisation-quite higher saving on the processing costsremains flexible at low temperatureshigh temperature resistanceelectrical insulator with v..
Maximum Service Temperature, Air 140 °C
284 °F
long term; EMS
EMS-Grivory Grivory® HT3Z LF black 9564 PA*
Product description: Grivory HT3Z LF is an unreinforced and impact resistant, PTFE modified engineering thermoplastic based on semi crystalline partially aromatic copolyamide. This Grivory HT produc..
Maximum Service Temperature, Air 140 °C
284 °F
long term; EMS
EMS-Grivory Grivory® HTM-4H1 PA6T/6I-MD40
Product description: Grivory HTM-4H1 is a 40 % mineral reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA ..
Maximum Service Temperature, Air 140 °C
284 °F
20000 h; VDE 0304/P2-1, IEC 216
EPICHEM Epilon PC GF 10 V0 Polycarbonate, 10% Glass Fiber
Characteristics: self-extinguishing V0 at 1,6 mm, 10% glass fibre filled
Maximum Service Temperature, Air 140 °C
284 °F
long term; EMS
EMS-Grivory Grivory® HT1V-4 FWA black 9225 PA6T/6I-GF40
Product description: Grivory HT1V-4 FWA black 9225 is a 40 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: ..
Maximum Service Temperature, Air 140 °C
284 °F
long term; EMS
EMS-Grivory Grivory® HT1V-5 FWA nat PA6T/6I-GF50
Product description: Grivory HT1V-5 FWA natural is a 50 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6..
Maximum Service Temperature, Air 140 °C
284 °F
long term; EMS
EMS-Grivory Grivory® HT2C-3X black 9833 PA6T/66-CF30
Product description: Grivory HT2C-3X black 9833 us a 30% carbon-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc to ISO: PA 6T/66...
Maximum Service Temperature, Air 140 °C
284 °F
at 50% loss of tensile strength after 5000h; IEC 216-1
BASF Ultradur B 4500 PBT
Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660.
Maximum Service Temperature, Air 140 °C
284 °F
short term
CENTROPLAST CENTROGUARD Polyoxymethylene, Antimicrobial
During the modification with POM CG, antimicrobial substances are included in the basic polyoxymethylene polymer, which provide an effective and long lasting solution against unwanted growth of micr..
Maximum Service Temperature, Air 140 °C
284 °F
for 50% loss of tensile strength after 5000hr
BASF Ultramid® A3HG5 LS BK 23189 25% Glass Filled PA66 (Dry)
Description: 25% glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used fo..
Maximum Service Temperature, Air 140 °C
284 °F
Short term
CENTROPLAST CENTRODAL C Polyoxymethylene Copolymer
CENTRODAL C is a versatile material with good chemical resistance, good machinability, and surface slip properties. Applications include sliding components and rollers, toothed wheels, ratchets, an..
Maximum Service Temperature, Air 140 °C
284 °F
RTI
Covestro Petlon® 3530 Semi-Crystalline PET, 30% Glass Fiber  (discontinued **)
Characteristics: Excellent Electrical Properties, High Heat and Chemical ResistanceApplications: Automotive (Underhood), Appliances, Casings and HousingsProcessing: Injection Molding (Melt Temperatu..
Maximum Service Temperature, Air 140 °C
284 °F
at 50% loss of tensile strength after 20000h; IEC 216-1
BASF Ultradur B 4300 G6 30% Glass Filled PBT
Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..
Maximum Service Temperature, Air 140 °C
284 °F
at 50% loss of tensile strength after 20000h; IEC 216-1
BASF Ultradur® B 4300 G10 50% Glass Filled PBT
Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou..
Maximum Service Temperature, Air 140 °C
284 °F
short term
Lehmann & Voss PLASLUBE NY-1/SI/2/NT Polyamide 66, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Information provided by Lehmann ..