| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | <= 100 °C | <= 212 °F | Hopper Temperature |
|
Victrex® PEEK 600G Polyetheretherketone
(discontinued **)
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta..
|
|||
| Processing Temperature | <= 100 °C | <= 212 °F | Hopper Temperature |
|
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou..
|
|||
| Processing Temperature | <= 100 °C | <= 212 °F | Hopper Temperature |
|
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c..
|
|||
| Processing Temperature | <= 100 °C | <= 212 °F | Hopper Temperature |
|
Victrex® PEEK 450FC30 General Purpose
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext..
|
|||
| Processing Temperature | <= 100 °C | <= 212 °F | Hopper Temperature |
|
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black
Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos..
|
|||
| Processing Temperature | <= 100 °C | <= 212 °F | Hopper Temperature |
|
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com..
|
|||
| Processing Temperature | 100 °C | 212 °F | Cure time 3 hr at this temperature. |
|
Momentive Performance Materials TSE3221 Clear Adhesive Sealant, Non-Corrosive Flowable
One-part heat cure. Typical uses: General sealing, potting, and coating when visual clarity is needed.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Perform..
|
|||
| Processing Temperature | 100 °C | 212 °F | Cure time 3 hr at this temperature. |
|
Momentive Performance Materials TSE322B Black Adhesive Sealant, Non-Corrosive Flowable
One-part heat cure. Typical uses: Thermal barrier for automotive parts. Fabric seam seal.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materia..
|
|||
| Processing Temperature | 100 °C | 212 °F | Cure time 2 hr at this temperature. |
|
Momentive Performance Materials TSE326 Red Adhesive Sealant, Non-Corrosive Flowable High Temperature
One-part heat cure. Typical uses: Assembly and gasketing.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materials in 2006.
|
|||
| Processing Temperature | 100 - 120 °C | 212 - 248 °F | conductor preheating temperature |
|
Borealis HE4872 High Density Polyethylene
HE4872 is a HDPE compound for solid insulation of symmetric data cable at high extrusion speed. Applications: high frequency data transmission cables, outer skin of foam-skin constructions. Specif..
|
|||
| Processing Temperature | 100 - 140 °C | 212 - 284 °F | Lamination Adhesive |
|
EMS-Griltech Griltex® D 1500A Copolyamide Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
|
|||
| Processing Temperature | 100 - 130 °C | 212 - 266 °F | Films Die Head |
|
EMS-Griltech Griltex® D 1531E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
|
|||
| Processing Temperature | 100 - 150 °C | 212 - 302 °F | Glue Line Temperature |
|
EMS-Griltech Griltex® D 1541A Copolyamide Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
|
|||
| Processing Temperature | 100 °C | 212 °F | Seal Initiation temperature |
|
Dow AFFINITY™ FM 1570 Polyolefin Plastomer
AFFINITY® FM 1570 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide film products with excellent sealability and high hot tack strength, outstanding blown film optics, and ..
|
|||
| Processing Temperature | 100 - 180 °C | 212 - 356 °F | extruder |
|
Fainplast Compounds Hax™ HF 411 Flame Retardant Polyolefin Cable Compound
Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:SheathingInformation provided by Fainplast Compounds
|
|||
| Processing Temperature | 100 - 180 °C | 212 - 356 °F | extruder |
|
Fainplast Compounds Hax™ HF 018/25 Flame Retardant Polyolefin Cable Compound
Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Insulation; very low thicknessInformation provided by Fainplast Compounds
|
|||
| Processing Temperature | 100 - 180 °C | 212 - 356 °F | extruder |
|
Fainplast Compounds Hax™ HF 039/4H Flame Retardant Polyolefin Cable Compound
Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Sheathing, insulation, high flexibilityInformation provided by Fainplast Compounds
|
|||
| Processing Temperature | 100 - 180 °C | 212 - 356 °F | extruder |
|
Fainplast Compounds Hax™ HF 225F Flame Retardant Polyolefin Cable Compound
Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Sheathing, high flexibilityInformation provided by Fainplast Compounds
|
|||
| Processing Temperature | 100 °C | 212 °F | Cure 4 hrs |
|
Aptek 2210A/B Electrically conductive urethane adhesive
Electrically conductive urethane adhesive, silver-filled, flexible low modulus, low outgassingAPTEK 2210-A/B is a two component, silver-filled, urethane adhesive designed for application where flexi..
|
|||
| Processing Temperature | 100 °C | 212 °F | Cure 5 hrs |
|
Aptek 2503R-A/B Premeasured conformal urethane coating repair kit
APTEK 2503-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the encapsulation and protection of electrical/electronic components..
|
|||
| Processing Temperature | 100 °C | 212 °F | Cure 0.5 hrs. |
|
Aptek 2712-A/B Very low stress silicone adhesive
Very low stress silicone adhesive; -110ºC to 260ºC operating range; Low outgassing/space gradeAPTEK 2712-A/B is a two component, white, very soft, thixotropic, electrically insulative, silicone ad..
|
|||
| Processing Temperature | 100 °C | 212 °F | Cure 0.75 hrs |
|
Aptek 6505PMF Electronic-grade, non-conductive adhesive
APTEK 6506-PMF is a one component, 100% solid, mineral-filled epoxy adhesive specifically designed for the attachment of electronic components to printed circuit boards as well as a protective barri..
|
|||
| Processing Temperature | 100 °C | 212 °F | Suggested baking time at this temperature is 0.25 hr. |
|
Von Roll Isola IMI Varnish 704 Solventless Polyester Varnish for Electrical Insulation
Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: 42°C. Usag..
|
|||
| Processing Temperature | <= 100 °C | <= 212 °F | Hopper Temperature |
|
Victrex® PEEK 150FC30 Easy Flow
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy ..
|
|||
| Processing Temperature | <= 100 °C | <= 212 °F | Hopper Temperature |
|
Victrex® PEEK 381G Medium Viscosity
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD..
|
|||
| Processing Temperature | <= 100 °C | <= 212 °F | Hopper Temperature |
|
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac..
|
|||
| Processing Temperature | <= 100 °C | <= 212 °F | Hopper Temperature |
|
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F..
|
|||