Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 232 - 270 °C | 450 - 518 °F | Average value: 251 °C Grade Count:9 |
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max.. |
|||
Processing Temperature | 80.0 - 270 °C | 176 - 518 °F | Average value: 151 °C Grade Count:5 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Processing Temperature | 240 - 270 °C | 464 - 518 °F | Injection molding cylinder temperature |
LG Chemical EG920 PMMA, General Purpose Grade for Extrusion General purpose grade with excellent stress cracking resistanceIntended mainly for exterior applicationsRecommended mainly for sheets, pipes, and profilesFeatures: Excellent transparency and eleganc.. |
|||
Processing Temperature | 160 - 270 °C | 320 - 518 °F | Coatings |
Lucobit Lucolit® 1323 Polyolefin TPO Granules, Green Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi.. |
|||
Processing Temperature | 230 - 270 °C | 446 - 518 °F | |
Gromax PBT 2100-104B Product Description: PBT unreinforced flame-retarded injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellen.. |
|||
Processing Temperature | 160 - 270 °C | 320 - 518 °F | Coatings |
Lucobit Lucofin® 1400SL Ethylene Butyl Acrylate Lucofin® 1400SL is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin® 1400SL is softer and more flexible than ethylene h.. |
|||
Processing Temperature | 240 - 270 °C | 464 - 518 °F | |
Ter Hell Plastic Terez® PA 6 7500 GF 30 Polyamide 6, 30% Glass Fiber Reinforced Description: Medium viscosity Polyamide 6, 30% glass fiber reinforced, good flowability, good impact resistance and bright natural color.Application: For molding parts with good stiffness and good.. |
|||
Processing Temperature | 225 - 270 °C | 437 - 518 °F | |
Zhejiang Juner PC Alloy Applications: Shell of Small Household Electric ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 225 - 270 °C | 437 - 518 °F | |
Zhejiang Juner PC/ABS Alloy Applications: Shell of Small Household Electric ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 250 - 270 °C | 482 - 518 °F | |
Eurotec® Tecodur® PB70 GB30 NL PBT, 30% glass bead reinforced, natural Information provided by Eurotec® |
|||
Processing Temperature | 250 - 270 °C | 482 - 518 °F | |
Eurotec® Tecodur® PB70 GR10 NL100 PBT, 10% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Processing Temperature | 250 - 270 °C | 482 - 518 °F | |
Eurotec® Tecodur® PB70 GR23 BK EF PBT, 23% glass fiber reinforced, black, suitable for electrostatic powder coating, gas injection grade Information provided by Eurotec® |
|||
Processing Temperature | 250 - 270 °C | 482 - 518 °F | |
Eurotec® Tecomid® NBX0 HF75 NL PA6, 75% heavy reinforced, improved flexibility, natural Information provided by Eurotec® |
|||
Processing Temperature | 250 - 270 °C | 482 - 518 °F | |
Eurotec® Tecodur® PB70 NL XA20 PBT, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Processing Temperature | 240 - 270 °C | 464 - 518 °F | Resin Temperature |
Asahi Kasei Xyron® 500Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Processing Temperature | 250 - 270 °C | 482 - 518 °F | |
Eurotec® Tecomid® NB40 GR25 NL PA6, 25% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Processing Temperature | 240 - 270 °C | 464 - 518 °F | |
Gromax CCP PBT 4830-BK 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Processing Temperature | 30.0 - 270 °C | 86.0 - 518 °F | Average value: 158 °C Grade Count:7 |
Overview of materials for Polypropylene with 60% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i.. |
|||
Processing Temperature | 30.0 - 270 °C | 86.0 - 518 °F | Average value: 208 °C Grade Count:20 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Processing Temperature | 160 - 270 °C | 320 - 518 °F | Coatings |
Lucobit Lucofin® 1414-t3 Polyolefin TPO Granules, Silk Grey Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t3 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and .. |