Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 70.0 - 340 °C | 158 - 644 °F | Average value: 233 °C Grade Count:9 |
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |
|||
Processing Temperature | 70.0 - 315 °C | 158 - 599 °F | Average value: 109 °C Grade Count:6 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
Processing Temperature | 70.0 - 293 °C | 158 - 560 °F | Average value: 181 °C Grade Count:6 |
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi.. |
|||
Processing Temperature | 70.0 - 100 °C | 158 - 212 °F | conductor preheating temperature; 2400 m/min line speed |
Borealis ME6032 Polypropylene ME6032 is a MDPE compound for solid insulation of telephone singles and data cables at high line speed. It contains a metal deactivator. Applications: Dry core and petroleum jelly filled cables. S.. |
|||
Processing Temperature | 70.0 - 80.0 °C | 158 - 176 °F | activation temperature used to laminate with a press or vacuum tube |
Gwent Electronic Materials R2040227D1 Hot Melt Conductive Adhesive for Diagnostic Sensors This is a one-component water based polyurethane dispersion used for bonding unsupported PVC foils. This can be used in many different diagnostic applications such as test cards, assays and support.. |
|||
Processing Temperature | 70.0 - 80.0 °C @Time 3600 sec |
158 - 176 °F @Time 1.00 hour |
|
Henkel Turco 5668 Deoxidizer Turco 5668 is a diphase, liquid paint remover developed to remove resistant coatings, such as aluminized silicones, polyurethanes, acrylics, epoxies and chromated primers without using phenols, chro.. |
|||
Processing Temperature | 70.0 - 270 °C | 158 - 518 °F | Average value: 135 °C Grade Count:9 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Processing Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
Henkel Turco 5668 Landing Gear Cleaner Turco 5668 is a diphase, liquid paint remover developed to remove resistant coatings, such as aluminized silicones, polyurethanes, acrylics, epoxies and chromated primers without using phenols, chro.. |