| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature |
80.0
-
90.0
°C @Time 1800 sec |
176
-
194
°F @Time 0.500 hour |
|
|
Henkel Turco Scale Gon 7 Jet Engine Cleaner
Turco Scale Gon 7 is an acid-activated, yellow liquid used in the Turco Jet Engine Process to condition and remove high temperature scale from jet engine parts. Approved by Rolls-Royce.Application: ..
|
|||
| Processing Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Homogenization (Calendering) |
|
Braskem PN2021 EVA Foam Copolymer
PN2021 is an Ethylene-Vinyl Acetate (EVA) copolymer mainly used for the production of crosslinked/expanded plates and other parts. It is a product with easy processability and high compatibility wit..
|
|||
| Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
|
Aremco Aremco-Seal™ 613 High Temperature Glass Coating
Glass-filled adhesive/sealer for use with porous ceramics and refractories to 1150 ºF (620 ºC)
|
|||
| Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
|
Aremco Aremco-Seal™ 617 High Temperature Glass Coating
Glass-filled adhesive/sealer for use with porous ceramics and refractories to 1500 ºF (816 ºC).
|
|||
| Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
|
Aremco Ceramabond™ 552 High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
|
|||
| Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
|
Aremco Ceramabond™ 571 High Temperature Ceramic Adhesive/Paste, Magnesium Oxide Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
|
|||
| Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
|
Aremco Ceramabond™ 600-N High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled
Aremco Ceramabond™ 600-N High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled
|
|||
| Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
|
Aremco Ceramabond™ 670 High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
|
|||
| Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
|
Aremco Ceramabond™ 671 High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
|
|||
| Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
|
Aremco Ceramabond™ 685-N High Temperature Ceramic Adhesive/Paste, Zirconia Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
|
|||
| Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
|
Aremco Ceramabond™ 835 High Temperature Ceramic Adhesive/Paste, Zirconia Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
|
|||
| Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
|
Aremco Ceramabond™ 835-MB High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
|
|||
| Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
|
Aremco HiE-Coat™ 840-C High Emissivity Coating, Inorganic-Ceramic Filled
Ceramic-based, black-pigmented coating for ceramic fiber modules and refactories to 2500°F (1371°C)
|
|||
| Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
|
Aremco HiE-Coat™ 840-CM High Emissivity Coating, Inorganic-Ceramic Filled
Ceramic-based, black-pigmented coating for dense refractories to 2500°F (1371°C) and stainless steel to 900°F (482°C)
|
|||
| Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
|
Aremco Pyro-Paint™ 634-ALP High Temperature Refractory Coating
This phosphate-bonded, alumina coating system bonds exceptionally well to dense refractory ceramics, providing high abrasion and corrosion resistance for operating temperatures to 3200°F (1760°C)
|
|||
| Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application |
|
Aremco Ceramabond™ 503 High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
|
|||
| Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
|
Aremco Ceramabond™ 569 High Temperature Ceramic Adhesive/Paste, Alumina Filled
White paste used for bonding of Ceramic-to-Ceramic; Ceramic-Metal; and Quartz. Used in Heaters, Igniters, Resistors, Sensors. This one component system air dries in 1-2 hrs and is ready for use fol..
|
|||
| Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
|
Aremco Ceramabond™ 668 High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
|
|||
| Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
|
Aremco Ceramabond™ 835-M High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
|
|||
| Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
|
Aremco Ceramabond™ 865 High Temperature Ceramic Adhesive/Paste, Aluminum Nitride Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
|
|||
| Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
|
Aremco Ceramabond™ 890 High Temperature Ceramic Adhesive/Paste, Silicon Carbide Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
|
|||
| Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
|
Aremco Graphi-Bond™ 669 High Temperature Ceramic Adhesive/Paste, Graphite Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
|
|||