Processing Properties Metric English Comments
Middle Barrel Temperature 210 °C
410 °F
Multibase Multi-Flex® V 5502 TPE Thermoplastic Polyolefin Elastomer
Forms: PelletsProcessing Methods:Injection Molding Features:Gloss, LowInformation provided by Multibase
Middle Barrel Temperature 210 - 238 °C
410 - 460 °F
RheTech Products FT4200-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Body side moldingsGrillesElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 210 - 238 °C
410 - 460 °F
RheTech Products FT5250-650UV Thermoplastic Polyolefin, UV Stabilized, Exterior 848 Black
Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 210 - 238 °C
410 - 460 °F
RheTech Products FT7013-720UV Thermoplastic Polyolefin, UV Stabilized, XTM Dark Sandstone
Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 210 - 238 °C
410 - 460 °F
RheTech Products FT7016-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 210 - 238 °C
410 - 460 °F
RheTech Products FT7016-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 210 - 238 °C
410 - 460 °F
RheTech Products GC30P103-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: Battery traysFender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 210 °C
410 °F
Zone 1; Cylinder
Premix Thermoplastics PRE-ELEC® PET 1451
PRE-ELEC PET 1451 is a conductive thermoplastic compound based on PETG. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PET 14..
Middle Barrel Temperature 210 - 232 °C
410 - 450 °F
Polymer Resources ABS-G30 ABS, 30% Glass Reinforced
Acrylonitrile Butadiene Styrene, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Middle Barrel Temperature 210 - 238 °C
410 - 460 °F
RheTech Products F25-01 34% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Support ductsHousingsBattery traysArm rest insertsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 210 - 232 °C
410 - 450 °F
PlastiComp Complet® LCF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Middle Barrel Temperature 210 - 232 °C
410 - 450 °F
PlastiComp Complet® LGF60 - TPU Rigid Thermoplastic Polyurethane, 60% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 60% long glass fiber reinforcementInformation provided by Plas..
Middle Barrel Temperature 210 - 232 °C
410 - 450 °F
Ineos Nova 879 High Performance Styrenic Enhanced Polystyrene  (discontinued **)
High heat crystal polystyrene, Color stable, Custom colorsApplications: Injection molding, Designed for applications requiring high strength, high heat resistance, and color stabilityPerformance gra..
Middle Barrel Temperature 210 - 230 °C
410 - 446 °F
Injection Molding
LG Chemical KEYFLEX BT GN7155F Ester Type TPE
Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical
Middle Barrel Temperature 210 - 240 °C
410 - 464 °F
Injection
Inno-Comp INNOPOL® CS 2-2130 30% Talc Filled Polypropylene Copolymer
INNOPOL® CS 2-2130 is a 30 % talc-filled polypropylene compound /PP-B TD30 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 2-2130 is recommended for produci..
Middle Barrel Temperature 210 °C
410 °F
Multibase Multi-Flex® 8832 C Black TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Middle Barrel Temperature 210 °C
410 °F
Multibase Multi-Flex® A 2599 TPE Thermoplastic Elastomer
This material bonds to polypropylene. Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame Retardant Flexibility, GoodHeat StabilizedOzone ResistantPr..
Middle Barrel Temperature 210 °C
410 °F
Multibase Multi-Flex® A 3540 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodSoftUV Resistance, Go..
Middle Barrel Temperature 210 °C
410 °F
Cast film
DuPont Elvaloy® 1609 AC Ethylene and 9% Methyl Acrylate Copolymer
Elvaloy® 1609 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®..
Middle Barrel Temperature 210 - 238 °C
410 - 460 °F
Clariant ABS4500 ABS, High Impact
Data provided by Clariant Masterbatches
Middle Barrel Temperature 210 - 240 °C
410 - 464 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s..
Middle Barrel Temperature 210 - 240 °C
410 - 464 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Middle Barrel Temperature 210 - 240 °C
410 - 464 °F
Tube Extrusion
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Middle Barrel Temperature 210 - 230 °C
410 - 446 °F
Injection Molding
LG Chemical XR401F ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Door Frame)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical
Middle Barrel Temperature 210 - 240 °C
410 - 464 °F
Tube Extrusion
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Middle Barrel Temperature 210 °C
410 °F
Cast film
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer  (discontinued **)
Elvaloy® 1126 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill..