Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Middle Barrel Temperature = 410 °F Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Middle Barrel Temperature 210 - 238 °C
410 - 460 °F
RheTech Products F43-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Fan shroudsDip trayFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 210 - 238 °C
410 - 460 °F
RheTech Products FT4200-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Body side moldingsGrillesElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 210 - 238 °C
410 - 460 °F
RheTech Products FT7016-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 210 - 238 °C
410 - 460 °F
RheTech Products G30P100-01 30% Glass Fiber Reinforced Polypropylene, Black
Applications: Fender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 210 - 238 °C
410 - 460 °F
RheTech Products GC30P103-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: Battery traysFender apronsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 210 - 232 °C
410 - 450 °F
PlastiComp Complet® LCF30 - TPU Rigid Thermoplastic Polyurethane, 30% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Middle Barrel Temperature 210 - 238 °C
410 - 460 °F
RheTech Products T30P100-00 30% Talc Reinforced Polypropylene, Natural
Applications: Headlamp housingsI/P componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 210 - 232 °C
410 - 450 °F
Ineos Nova 2124 High Performance Styrenic Enhanced Polystyrene  (discontinued **)
Appearance comparable to ABS, High gloss at 60°=95; at 20°=90, Significantly reduced stress whitening, custom colors, UL94 HB at 0.62 for all colorsApplications: Injection molding, Toys, Small app..
Middle Barrel Temperature 210 - 230 °C
410 - 446 °F
Injection Molding
LG Chemical KEYFLEX BT GN7155F Ester Type TPE
Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical
Middle Barrel Temperature 210 - 227 °C
410 - 440 °F
MRC Polymers MAXTELâ„¢ 600 GF30 TPO, 30% Glass Fiber Filled
For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc.
Middle Barrel Temperature 210 °C
410 °F
Multibase Multi-Flex® A 1540 Natural TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodSoftUV Resistance, Go..
Middle Barrel Temperature 210 °C
410 °F
Multibase Multi-Flex® A 3005 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHardness, LowFoamableHeat StabilizedGeneral PurposeOzone ResistantProce..
Middle Barrel Temperature 210 °C
410 °F
Multibase Multi-Flex® A 7011 TPE Thermoplastic Elastomer
This material bonds to polypropylene.Forms:PelletsProcessing Method:Injection Molding Information provided by Multibase
Middle Barrel Temperature 210 °C
410 °F
Multibase Multi-Flex® A 8502 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Heat StabilizedOzone ResistantGeneral Purpose Moldability, GoodPaintable Forms:PelletsProcessing Method:Injection Molding Uses: Automotive Interior PartsInforma..
Middle Barrel Temperature 210 °C
410 °F
Multibase Multi-Flex® D 2010 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good F..
Middle Barrel Temperature 210 °C
410 °F
Cast film
DuPont Elvaloy® 1209 AC Ethylene and 9% Methyl Acrylate Copolymer
Elvaloy® 1209 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®..
Middle Barrel Temperature 210 °C
410 °F
Cast film
DuPont Elvaloy® 1609 AC Ethylene and 9% Methyl Acrylate Copolymer
Elvaloy® 1609 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®..
Middle Barrel Temperature 210 °C
410 °F
Beijing Chemical Industry KAIFA® GL3300 ABS Flame-Retardant Grade
Good flammabilityInformation provided by Beijing Chemical Industry Research Institute (Group)
Middle Barrel Temperature 210 - 221 °C
410 - 430 °F
A. Schulman ComAlloy Voloy® 100 Polypropylene, Mineral Reinforced, Flame Retardant, UL, CSA
Data provided by the manufacturer, ComAlloy International Company.15% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 210 - 221 °C
410 - 430 °F
A. Schulman ComAlloy Voloy® 110 Polypropylene, Mineral Reinforced, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.15% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 210 - 238 °C
410 - 460 °F
RheTech Products GC30P104-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: BracketsHead lamp housingsBattery trayInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 210 °C
410 °F
Cast film
DuPont Elvaloy® 3107 AC Ethylene and 7% Butyl Acrylate Copolymer  (discontinued **)
Elvaloy® 3107 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3107 AC is developed to give films with good sealing properties, impact strength at lower temperature, and low shrinkag..
Middle Barrel Temperature 210 - 230 °C
410 - 446 °F
Injection Molding
LG Chemical XR401F ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Door Frame)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical
Middle Barrel Temperature 210 - 230 °C
410 - 446 °F
Injection Molding
LG Chemical XR404T ABS, Heat Resistance
Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9, and 9001-96-2Information provided by LG Chemical..
Copyright © lookpolymers.com All Rights Reserved